DLL = Linear thermal expansion (ΔL/L) |
MTE = Mean coefficient of thermal expansion |
CTE = Coefficient of thermal expansion |
D = Density |
AV = Apparent viscosity | |
|
TC = Thermal conductivity |
SH = Specific heat |
HC = Heat capacity |
TD = Thermal diffusivity |
SV = Specific volume | |
|
RHO = Electrical resistivity |
SIGMA = Electrical conductivity |
SRHO = Surface electrical resistivity |
Vis = Viscosity |
FS = Flexural strength | |
|
E = Elastic/Young's modulus |
G = Shear modulus |
v = Poisson's ratio |
K = Bulk modulus |
FM = Flexural modulus | |
|
SSC = True stress-strain curve (tension) |
SSCC = True stress-strain curve (compression) |
HE = Hemispherical total emissivity |
NE = Normal total emissivity |
ESSC = Engineering stress-strain curve (tension) | |
|
UTS = Tensile strength |
YS = Yield strength (tension) |
UCS = Compressive strength |
YSC = Yield strength (compression) |
%El = Elongation | |
|
FSN = Fatigue S-N curve |
FEN = Fatigue ε-N curve |
SR = Stress rupture |
CRS = Creep strength |
ESSCC = Engineering stress-strain curve (compression) | |
|
RPB = Relative permeability |
AP = Absolute permeability |
BH = B-H curve |
HB = H-B curve |
CRM = Creep modulus | |
|
DCRPT = Relative permittivity |
DF = Dissipation factor |
CL = Core loss |
EP = Exciting Power |
IC = Isochronous creep | |
|
RIW = Refractive index vs λ |
RIT = Refractive index vs T |
TWL = Transmission vs λ |
ST = Surface tension |
CRR = Stress vs Creep rate | |
|
S = Seebeck coefficient |
VP = Vapor pressure |
| 2020 | 2090 | 5083 | 5251 | 7075 |
| 8090 | 2091 (New) | 46 Al - 33 Cu - 21 Zn (wt%) | Al - 3 Li - 1.25 Mn (wt %) (11 a/o Li) (New) | Al - 0.6 Li (wt %) (2.3 a/o Li) |
| Al - 2.5 Li (wt %) (9 a/o Li) (New) | Al - 2.1 Li (wt %) (7.7 a/o Li) (Revised) | Al - 0.22 Mn (at %) (New) | Al - 0.35 Mn (at %) (New) | Al - 0.5 Mn (at %) (New) |
| Al - 1 Mn (at %) (New) | Al - 2 Mn (at %) (New) | Al - 0.062 Mn (at %) (New) | Al - 6 Zn - 2 Mg - 0.5 Ni - 0.3 Fe (wt %) | Al - 5 Zn - 3 Mg - 0.1 Zr (wt %) (New) |
| Al - 20 Zn (wt %) (New) | Al - 40 Zn (wt %) (New) |
| AlB2 | CoB | Co2B | Fe2B | FeB |
| MgB4 | MnB | Mn2B | Mn3B4 | NiB |
| Ni2B | Ni3B | TiB | V3B4 | VB |
| V2B3 | V3B2 |
| MgC2 | Mg2C3 | Mn23C6 | Mn3C | Mn7C3 |
| MoC | Nb4C3 | Ni3C | SrC2 |
| Graphite AXF-5Q | Graphite MPG-6 |
| EuFeO3 | EuPd2As2 | GaFeO3 (Sm doped) | LaCrO3 (Ca & Sr doped) | LaFeO3 |
| LaRhO3 | LiIn | Mn3CuN | NdCoO3 |
| Antimony | Arsenic | Barium (Revised) | Bismuth (Revised) | Cadmium (Revised) |
| Caesium | Calcium | Chromium (Revised) | Europium | Gadolinium (Revised) |
| Gallium (Revised) | Gold | Hafnium | Holmium (Revised) | Indium (Revised) |
| Iron | Lanthanum (Revised) | Lead (Revised) | Lithium (Revised) | Magnesium (Revised) |
| Mercury | Molybdenum (Revised) | Neodymium (Revised) | Nickel (Revised) | Niobium (Revised) |
| Palladium (Revised) | Praseodymium | Rubidium | Samarium | Strontium |
| Tantalum (Revised) | Terbium (Revised) | Thorium (Revised) | Titanium (Revised) | Tungsten (Revised) |
| Vanadium (Revised) | Ytterbium | Yttrium | Zinc | Zirconium (Revised) |
| Cheddar cheese |
| GdNiH3.2 (New) | Pd - H (New) | SrH2 | ThH2 |
| AZ91 | Mg - 79 Ca (wt %) (New) | Mg - 4 Li - 5 Al (wt %) | Mg - 4 Li - 3 Al (wt %) | Mg - 21 Li (at %) |
| Mg - 25 Li (at %) | Mg - 30 Li (at %) | Mg - 12.7 Li (at %) | Mg - 32 Li (at %) (New) | Mg - 1 Si (wt %) |
| ZK60 |
| Ca - 40 Al - 10 Ga (at %) (New) | Ca - 40 Al - 20 Ga (at %) (New) | Ca - 30 Al (at %) (New) | Ca - 33 Al (at %) (New) | Ca - 40 Al (at %) (New) |
| Ca - 45 Al (at %) (New) | Ca - 20 Al (at %) (New) | Ca - 25 Al (at %) (New) | Co80P20 (New) | Co77P23 (New) |
| Co76P24 (New) | Cu60Hf40 (New) | Cu43Ti57 (New) | Cu66Ti34 (New) | Cu55Ti45 (New) |
| Cu45Zr55 (New) | Cu27.5Zr72.5 (New) | Cu60Zr40 (New) | Cu50Zr50 (New) | Cu50Zr40Fe10 (New) |
| (Fe1-xCox)90Zr10 (New) | Fe32Ni36Cr14P12B6 (New) | Fe40Ni40P14B8 (New) | (Fe1-xNix)90Zr10 (New) | Fe79P21 (New) |
| La - 18 Al (at %) (New) | La - 20 Al (at %) (New) | La - 25 Al (at %) (New) | La - 28 Al (at %) (New) | Mg - 30 Zn (at %) |
| Mg - 25 Zn (at %) (New) | Mg - 20 Zn (at %) (New) | Mg - 33 Zn (at %) (New) | Mg - 35 Zn (at %) (New) | Ni0.595Nb0.405 |
| Ni65Nb35 (New) | Ni66Nb34 (New) | Ni64Zr36 (New) | Ni37Zr63 (New) | Ni24Zr76 (New) |
| Pd80Si20 (New) | Rh60B32Si8 (New) | Rh65B27Si8 (New) | Rh70B22Si8 (New) | Ti50Be40Zr10 (New) |
| Zr0.8Fe0.2 (New) | Zr64Ni36 |
| CrN | Cr2N | Fe2N | Fe4N | Mn3N2 |
| Nd2AlO3N | Sr2TaO3N | Ta2N | ThN | Th3N4 |
| VN | Zn3N2 |
| C4F9OCH3 (Novec 71000) (New) | C10H16 (alpha-pinene) (New) | C10H16 (beta-pinene) (New) | C2H6 (ethane) (Revised) | C2H2F4 (HFC-134a) |
| C3H2F6 (HFC-236ea) | C10H16O (limonene oxide) (New) |
| Pr6O11 | Ti3O5 |
| 3.33 CaCl2 - 6.67 NaCl - 90 H2O (wt %) (New) | 5 CaCl2 - 10 NaCl - 85 H2O (wt %) (New) | 6.67 CaCl2 - 13.33 NaCl - 80 H2O (wt %) (New) | 1.67 CaCl2 - 3.33 NaCl - 95 H2O (wt %) (New) |
| 28.9 KF - 71.1 LiF (mol %) (New) | 48.8 KF - 51.2 LiF (mol %) (New) |
| LiBr | NaBr | NaCl (Revised) | PaBr4 | PaCl4 |
| PaCl5 | TiBr3 | TlCl |
| CaF2 (Revised) | NaF | NpF3 | PbF2 | TiI3 |
| CoS2 | Co3S4 | CrS | DyS1.48 (New) | GdS1.48 (New) |
| InS | MnS2 | Mo2S3 | Ni3S4 | NiS2 |
| OsS2 | Pd4S | PtS2 | PtS | ThS2 |
| ThS | TiS |
| 2 CaCl2 - 4 MgCl2 - 4 NaCl - 90 H2O (wt %) (New) | 5 CaCl2 - 5 MgCl2 - 5 NaCl - 85 H2O (wt %) (New) | 5 CaCl2 - 5 MgCl2 - 10 NaCl - 80 H2O (wt %) (New) | 1 CaCl2 - 2 MgCl2 - 2 NaCl - 95 H2O (wt %) (New) |
| AlOCl | Cd3As2 | CdS | Co3Se4 | CrGe |
| Cr11Ge19 | CrSb2 | Cu1.8Mo6S8 (New) | Cu1.8Mo6Se8 (New) | Cu1.8Mo6S5Se3 (New) |
| Cu1.8Mo6S4Se4 (New) | Cu1.8Mo6S3Se5 (New) | Cu1.8Mo6S2Se6 (New) | Cu1.8Mo6SSe7 (New) | Cu1.8Mo6S7Se (New) |
| Cu1.8Mo6S6Se2 (New) | Cu1.8Mo6S4Te4 (New) | Cu1.8Mo6S7Te (New) | Cu1.8Mo6S6Te2 (New) | Cu1.8Mo6S5Te3 (New) |
| EuP | EuTe | FeSb2 | FeSe | FeTe2 |
| GaAs | GaP (Revised) | Ga2Se3 | GaTe | GdP |
| GeAs | GeSe2 | HgCr2Se4 (Revised) | InAs | InSe (Mn doped) |
| InTe | Mn3P | MnP | Mn2P | MnSe |
| Mo3P | Mo3Se4 | Mo3Te4 | NiSe2 | NiTe |
| PdTe2 | RuSe2 | RuTe2 | SnS2 | SnSe2 |
| TlSe | YbRh1.4Sn4.6 (New) | ZnS (Revised) | ZnSb | ZrTe2 |
| Cr3Si | Cr5Si3 | CrSi | Fe1.8Mn1.2Si (New) | Fe1.4Mn1.6Si (New) |
| Fe2.4Mn0.6Si (New) | Fe2.2Mn0.8Si (New) | Fe2MnSi (New) | FeSi2 | Fe3Si (Revised) |
| MnSi | Mn3Si | Mn5Si3 | Mo3Si | MoSi2 |
| Nb5Si3 | NdFe2Si2 | Ni2Si | NiSi | Pr5Si3 |
| WSi2 | W5Si3 | Y3RhSi3 | Y3Rh2Si3 |
| DOWSIL 550 fluid (Revised) |
| AgTl3Te2 | AuSe | Bi2Te2S | CaCu3Ti4O12 | CaZn2Sb2 |
| CeRu4Sn6 | CsCaBi (New) | CuFeS2 | Cu5FeS4 | EuZn2Sb2 |
| Fe2TiSn | Fe2VAl | Fe2V1-xAl1+x | GdxDy1-xS1.5 (New) | HfNiSn |
| KCaBi (New) | MgAgSb | MnTe | NdFe4Sb12 | PbTe (Revised) |
| PtSb2 (Te doped) | RbCaBi (New) | RuGa3 | Ru25Ga75-xZnx | Sr2IrO4 |
| TlBiTe2 | Tl3GeTe3 | TlInTe2 | TlSbTe2 | Zn - 40 Sb (at %) (New) |
| Zn - 43 Sb (at %) (New) | Zn - 50 Sb (at %) (New) | Zn - 60 Sb (at %) (New) | Zn - 70 Sb (at %) (New) | Zn - 80 Sb (at %) (New) |
| Zn - 90 Sb (at %) (New) | Zn - 10 Sb (at %) (New) | Zn - 20 Sb (at %) (New) | Zn - 30 Sb (at %) (New) | ZnSb (Cd, Pb, & Sn doped) |
| Zn4Sb3 (Zn13Sb10) (Na & Mg doped) |
| Ti - 33 Al - 3 Mn (wt %) (New) | Ti - 6 Al - 2 Sn - 4 Zr - 6 Mo (wt %) | Ti - 33 Al - 5 Zr (wt %) (New) | Ti - 33.5 Al (wt %) (New) | Ti - 0.3 Mo - 0.8 Ni (Grade 12) (Revised) |
| Ti - 0.05 Pd (Grade 17) (Revised) | Ti - 0.15 Pd (Grade 11) (Revised) | Ti - 0.15 Pd (Grade 7) (Revised) | Ti - 0.05 Pd (Grade 16) (Revised) | Ti - 0.1 Ru (Grade 27) (Revised) |
| Ti - 0.1 Ru (Grade 26) (Revised) | Ti - 40 V (wt %) | Ti - 13 V (wt %) | Ti - 26 V (wt %) | Ti - 30 V (wt %) |
| Ti - 32 V (wt %) | Ti Grade 4 (Revised) | Ti Grade 1 (Revised) | Ti Grade 2 (Revised) | Ti Grade 3 (Revised) |
| Timetal 685 |
| T6 (New) |
1018
SSCC (N): 0.25/s || tested at 900 °C (1652 °F) || 0 to 1.7 mm/mm strain
SSCC (N): 0.25/s || tested at 1000 °C (1832 °F) || 0 to 1.56 mm/mm strain
SSCC (N): 0.25/s || tested at 1100 °C (2012 °F) || 0 to 2 mm/mm strain
SSCC (N): 2.5/s || tested at 900 °C (1652 °F) || 0 to 1.67 mm/mm strain
SSCC (N): 2.5/s || tested at 1000 °C (1832 °F) || 0 to 1.5 mm/mm strain
SSCC (N): 2.5/s || tested at 1100 °C (2012 °F) || 0 to 1.9 mm/mm strain
SSCC (N): 25/s || tested at 900 °C (1652 °F) || 0 to 1.5 mm/mm strain
SSCC (N): 25/s || tested at 1000 °C (1832 °F) || 0 to 1.65 mm/mm strain
SSCC (N): 25/s || tested at 1100 °C (2012 °F) || 0 to 1.7 mm/mm strain
return to listing
1045
UTS (N*): quenched & tempered || as-quenched, 719 BHN || room temperature value
UTS (N*): quenched & tempered || tempered at 182 °C (360 °F), 630 BHN || room temperature value
UTS (N*): quenched & tempered || tempered at 260 °C (500 °F), 555 BHN || room temperature value
UTS (N*): quenched & tempered || tempered at 316 °C (600 °F), 488 BHN || room temperature value
UTS (N*): quenched & tempered || tempered at 382 °C (720 °F), 416 BHN || room temperature value
YS (N*): quenched & tempered || as-quenched, 719 BHN || room temperature value
YS (N*): quenched & tempered || tempered at 182 °C (360 °F), 630 BHN || room temperature value
YS (N*): quenched & tempered || tempered at 260 °C (500 °F), 555 BHN || room temperature value
YS (N*): quenched & tempered || tempered at 316 °C (600 °F), 488 BHN || room temperature value
YS (N*): quenched & tempered || tempered at 382 °C (720 °F), 416 BHN || room temperature value
%El (N*): quenched & tempered || as-quenched, 719 BHN || room temperature value
%El (N*): quenched & tempered || tempered at 182 °C (360 °F), 630 BHN || room temperature value
%El (N*): quenched & tempered || tempered at 260 °C (500 °F), 555 BHN || room temperature value
%El (N*): quenched & tempered || tempered at 316 °C (600 °F), 488 BHN || room temperature value
%El (N*): quenched & tempered || tempered at 382 °C (720 °F), 416 BHN || room temperature value
FSN (N): normalized || tested at 20 °C (68 °F), R = -1, axial, 80 Hz, stress amplitude || 1 x 105 cycles to 5 x 105 cycles
FSN (N): normalized || tested at 20 °C (68 °F), R = -1, axial, 260 Hz, stress amplitude || 5 x 104 cycles to 2 x 106 cycles
FSN (N): quenched & tempered || tested at 20 °C (68 °F), R = -1, axial, as-quenched, 719 BHN, stress amplitude || 1 cycles to 3 x 105 cycles
FSN (N): quenched & tempered || tested at 20 °C (68 °F), R = -1, axial, tempered at 182 °C (360 °F), 630 BHN, stress amplitude || 1 cycles to 5 x 105 cycles
FSN (N): quenched & tempered || tested at 20 °C (68 °F), R = -1, axial, tempered at 260 °C (500 °F), 555 BHN, stress amplitude || 1 cycles to 2 x 103 cycles
FSN (N): quenched & tempered || tested at 20 °C (68 °F), R = -1, axial, tempered at 316 °C (600 °F), 488 BHN, stress amplitude || 1 cycles to 1.5 x 104 cycles
FSN (N): quenched & tempered || tested at 20 °C (68 °F), R = -1, axial, tempered at 382 °C (720 °F), 416 BHN, stress amplitude || 1 cycles to 2.3 x 104 cycles
return to listing
1065
SH (N): solid || 20 °C (68 °F) to 675 °C (1247 °F)
TD (N): solid || 20 °C (68 °F) to 675 °C (1247 °F)
return to listing
1075
SH (N): solid || 20 °C (68 °F) to 675 °C (1247 °F)
TD (N): solid || 20 °C (68 °F) to 675 °C (1247 °F)
return to listing
301
FSN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, stress amplitude || 2.8 x 103 cycles to 1.5 x 106 cycles
FSN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 10% pre-strain, stress amplitude || 4.2 x 103 cycles to 1.6 x 106 cycles
FEN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 0.04/s, total strain amplitude || 2.8 x 103 cycles to 1.5 x 106 cycles
FEN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 0.04/s, plastic strain amplitude || 2.8 x 103 cycles to 1.5 x 106 cycles
FEN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 0.04/s, elastic strain amplitude || 2.8 x 103 cycles to 1.5 x 106 cycles
FEN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 0.04/s, 10% pre-strain, total strain amplitude || 4.2 x 103 cycles to 1.6 x 106 cycles
FEN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 0.04/s, 10% pre-strain, plastic strain amplitude || 4.2 x 103 cycles to 1.6 x 106 cycles
FEN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 0.04/s, 10% pre-strain, elastic strain amplitude || 4.2 x 103 cycles to 1.6 x 106 cycles
return to listing
316
UTS (N*): effect of aging time on room temperature value || as-received, not aged || room temperature value
UTS (N*): effect of aging time on room temperature value || aged 19 h at 700 °C (1292 °F) || room temperature value
UTS (N*): effect of aging time on room temperature value || aged 161 h at 700 °C (1292 °F) || room temperature value
UTS (N*): effect of aging time on room temperature value || aged 1068 h at 700 °C (1292 °F) || room temperature value
UTS (N*): effect of aging time on room temperature value || aged 4380 h at 700 °C (1292 °F) || room temperature value
YS (N*): effect of aging time on room temperature value || as-received, not aged || room temperature value
YS (N*): effect of aging time on room temperature value || aged 19 h at 700 °C (1292 °F) || room temperature value
YS (N*): effect of aging time on room temperature value || aged 161 h at 700 °C (1292 °F) || room temperature value
YS (N*): effect of aging time on room temperature value || aged 1068 h at 700 °C (1292 °F) || room temperature value
YS (N*): effect of aging time on room temperature value || aged 4380 h at 700 °C (1292 °F) || room temperature value
%El (N*): effect of aging time on room temperature value || as-received, not aged || room temperature value
%El (N*): effect of aging time on room temperature value || aged 19 h at 700 °C (1292 °F) || room temperature value
%El (N*): effect of aging time on room temperature value || aged 161 h at 700 °C (1292 °F) || room temperature value
%El (N*): effect of aging time on room temperature value || aged 1068 h at 700 °C (1292 °F) || room temperature value
%El (N*): effect of aging time on room temperature value || aged 4380 h at 700 °C (1292 °F) || room temperature value
return to listing
2205
FSN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, stress amplitude || 1.1 x 104 cycles to 1.9 x 106 cycles
FEN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 0.04/s, total strain amplitude || 1.1 x 104 cycles to 1.9 x 106 cycles
FEN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 0.04/s, plastic strain amplitude || 1.1 x 104 cycles to 1.9 x 106 cycles
FEN (N): annealed || tested at 20 °C (68 °F), R = -1, axial, 0.04/s, elastic strain amplitude || 1.1 x 104 cycles to 1.9 x 106 cycles
return to listing
2020
FEN (N): T651 temper || tested at 25 °C (77 °F), R = -1, axial, tested in air and vacuum, plastic strain amplitude || 4.5 cycles to 1.8 x 103 cycles
FEN (N): T651 temper || tested at 160 °C (320 °F), R = -1, axial, tested in vacuum, plastic strain amplitude || 32 cycles to 780 cycles
FEN (N): T651 temper || tested at 160 °C (320 °F), R = -1, axial, tested in air, plastic strain amplitude || 30 cycles to 620 cycles
FEN (N): T6X51 temper || tested at 25 °C (77 °F), R = -1, axial, tested in air and vacuum, plastic strain amplitude || 5.4 cycles to 3.8 x 103 cycles
FEN (N): T6X51 temper || tested at 160 °C (320 °F), R = -1, axial, tested in vacuum, plastic strain amplitude || 230 cycles to 1.4 x 103 cycles
FEN (N): T6X51 temper || tested at 160 °C (320 °F), R = -1, axial, tested in air, plastic strain amplitude || 220 cycles to 1.1 x 103 cycles
return to listing
5083
E (N*): H111 temper, sheet || rolling direction || room temperature value
E (N*): H111 temper, sheet || transverse direction || room temperature value
SSC (N): O temper, plate || tested at -196.1 °C (-321.1 °F), unknown strain rate || 0 to 0.36 mm/mm strain
SSC (N): H111 temper, 4 mm (0.157 inch) sheet || tested at 22 °C (72 °F), rolling direction, quasi-static strain rate || 0 to 0.19 mm/mm strain
SSC (N): H111 temper, 4 mm (0.157 inch) sheet || tested at 22 °C (72 °F), transverse direction, quasi-static strain rate || 0 to 0.19 mm/mm strain
UTS (N*): H111 temper, sheet || rolling direction || room temperature value
UTS (N*): H111 temper, sheet || transverse direction || room temperature value
YS (N*): H111 temper, sheet || rolling direction || room temperature value
YS (N*): H111 temper, sheet || transverse direction || room temperature value
%El (N*): H111 temper, sheet || rolling direction || room temperature value
%El (N*): H111 temper, sheet || transverse direction || room temperature value
FSN (N): H111 temper, 4 mm (0.157 inch) sheet || tested at 22 °C (72 °F), R = 0.1, axial, rolling direction, stress amplitude || 1 x 105 cycles to 1 x 108 cycles
FSN (N): H111 temper, 4 mm (0.157 inch) sheet || tested at 22 °C (72 °F), R = 0.1, axial, transverse direction, stress amplitude || 1 x 105 cycles to 1 x 108 cycles
return to listing
7075
SSCC (N): as-cast || tested at 25 °C (77 °F), 1300/s || 0 to 0.15 mm/mm strain
SSCC (N): as-cast || tested at 100 °C (212 °F), 1300/s || 0 to 0.15 mm/mm strain
SSCC (N): as-cast || tested at 200 °C (392 °F), 1300/s || 0 to 0.15 mm/mm strain
SSCC (N): as-cast || tested at 300 °C (572 °F), 1300/s || 0 to 0.15 mm/mm strain
SSCC (N): as-cast || tested at 25 °C (77 °F), 3100/s || 0 to 0.33 mm/mm strain
SSCC (N): as-cast || tested at 100 °C (212 °F), 3100/s || 0 to 0.31 mm/mm strain
SSCC (N): as-cast || tested at 200 °C (392 °F), 3100/s || 0 to 0.3 mm/mm strain
SSCC (N): as-cast || tested at 300 °C (572 °F), 3100/s || 0 to 0.31 mm/mm strain
SSCC (N): T6 temper || tested at 25 °C (77 °F), 1300/s || 0 to 0.15 mm/mm strain
SSCC (N): T6 temper || tested at 100 °C (212 °F), 1300/s || 0 to 0.15 mm/mm strain
SSCC (N): T6 temper || tested at 200 °C (392 °F), 1300/s || 0 to 0.15 mm/mm strain
SSCC (N): T6 temper || tested at 300 °C (572 °F), 1300/s || 0 to 0.15 mm/mm strain
SSCC (N): T6 temper || tested at 25 °C (77 °F), 3100/s || 0 to 0.36 mm/mm strain
SSCC (N): T6 temper || tested at 100 °C (212 °F), 3100/s || 0 to 0.23 mm/mm strain
SSCC (N): T6 temper || tested at 200 °C (392 °F), 3100/s || 0 to 0.3 mm/mm strain
SSCC (N): T6 temper || tested at 300 °C (572 °F), 3100/s || 0 to 0.3 mm/mm strain
return to listing
2091 (New)
D (*): solid || room temperature value
E (*): T351 temper || parallel to rolling direction || room temperature value
E (*): T351 temper || 90° to rolling direction || room temperature value
UTS (*): T351 temper || parallel to rolling direction || room temperature value
UTS (*): T351 temper || 90° to rolling direction || room temperature value
UTS (*): T8 temper || parallel to rolling direction || room temperature value
UTS (*): T8 temper || 45° to rolling direction || room temperature value
UTS (*): T8 temper || 90° to rolling direction || room temperature value
UTS (*): T81 temper || parallel to rolling direction || room temperature value
UTS (*): T81 temper || 45° to rolling direction || room temperature value
UTS (*): T81 temper || 90° to rolling direction || room temperature value
YS (*): T351 temper || parallel to rolling direction || room temperature value
YS (*): T351 temper || 90° to rolling direction || room temperature value
YS (*): T8 temper || parallel to rolling direction || room temperature value
YS (*): T8 temper || 45° to rolling direction || room temperature value
YS (*): T8 temper || 90° to rolling direction || room temperature value
YS (*): T81 temper || parallel to rolling direction || room temperature value
YS (*): T81 temper || 45° to rolling direction || room temperature value
YS (*): T81 temper || 90° to rolling direction || room temperature value
UCS (*): T351 temper || parallel to rolling direction || room temperature value
UCS (*): T351 temper || 90° to rolling direction || room temperature value
YSC (*): T351 temper || parallel to rolling direction || room temperature value
YSC (*): T351 temper || 90° to rolling direction || room temperature value
%El (*): T351 temper || parallel to rolling direction || room temperature value
%El (*): T351 temper || 90° to rolling direction || room temperature value
%El (*): T8 temper || parallel to rolling direction || room temperature value
%El (*): T8 temper || 45° to rolling direction || room temperature value
%El (*): T8 temper || 90° to rolling direction || room temperature value
%El (*): T81 temper || parallel to rolling direction || room temperature value
%El (*): T81 temper || 45° to rolling direction || room temperature value
%El (*): T81 temper || 90° to rolling direction || room temperature value
FSN : T351 temper || tested at 20 °C (68 °F), R = 0.1, axial, maximum stress || 2.7 x 104 cycles to 1 x 109 cycles
FSN : T81 temper || tested at 20 °C (68 °F), R = 0.05, axial, maximum stress || 1.3 x 105 cycles to 1 x 107 cycles
FSN : T621 temper || tested at 20 °C (68 °F), R = 0.05, axial, maximum stress || 6 x 104 cycles to 1 x 107 cycles
return to listing
Ag - 0.007 As (wt %) (New)
S : solid || alpha phase || -253.1 °C (-423.7 °F) to -63 °C (-82 °F)
return to listing
Ag - 0.042 As (wt %) (New)
S : solid || alpha phase || -253.1 °C (-423.7 °F) to -63 °C (-82 °F)
return to listing
Ag - 0.35 As (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -63 °C (-82 °F)
return to listing
Ag - 2.2 As (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -63 °C (-82 °F)
return to listing
Ag - 0.05 Cu (wt %) (New)
S : solid || alpha phase || -261.1 °C (-438.1 °F) to -63 °C (-82 °F)
return to listing
Ag - 0.5 Cu (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -63 °C (-82 °F)
return to listing
Ag - 0.01 Ga (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -73 °C (-100 °F)
return to listing
Ag - 0.05 Ga (wt %) (New)
S : solid || alpha phase || -257.1 °C (-430.9 °F) to -73 °C (-100 °F)
return to listing
Ag - 0.2 Ga (wt %) (New)
S : solid || alpha phase || -263.1 °C (-441.7 °F) to -73 °C (-100 °F)
return to listing
Ag - 1.6 Ga (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -83 °C (-118 °F)
return to listing
Ag - 6.6 Ga (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -83 °C (-118 °F)
return to listing
Ag - 0.04 Ge (wt %) (New)
S : solid || alpha phase || -257.1 °C (-430.9 °F) to -63 °C (-82 °F)
return to listing
Ag - 0.2 Ge (wt %) (New)
S : solid || alpha phase || -263.1 °C (-441.7 °F) to -63 °C (-82 °F)
return to listing
Ag - 0.57 Ge (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -63 °C (-82 °F)
return to listing
Ag - 2 Ge (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -63 °C (-82 °F)
return to listing
Ag - 1 Pd (wt %)
RHO (N): liquid || 979 °C (1794 °F) to 1479 °C (2694 °F)
SIGMA (N): liquid || 979 °C (1794 °F) to 1479 °C (2694 °F)
return to listing
Ag - 3 Pd (wt %)
RHO (N): liquid || 992 °C (1817 °F) to 1492 °C (2717 °F)
SIGMA (N): liquid || 992 °C (1817 °F) to 1492 °C (2717 °F)
return to listing
Ag - 5 Pd (wt %)
RHO (N): liquid || 1015 °C (1859 °F) to 1515 °C (2759 °F)
SIGMA (N): liquid || 1015 °C (1859 °F) to 1515 °C (2759 °F)
return to listing
Ag - 15 Pd (wt %)
RHO (N): liquid || 1101 °C (2014 °F) to 1601 °C (2914 °F)
SIGMA (N): liquid || 1101 °C (2014 °F) to 1601 °C (2914 °F)
return to listing
Ag - 25 Pd (wt %)
RHO (N): liquid || 1183 °C (2161 °F) to 1683 °C (3061 °F)
SIGMA (N): liquid || 1183 °C (2161 °F) to 1683 °C (3061 °F)
return to listing
Ag - 35 Pd (wt %)
RHO (N): liquid || 1255 °C (2291 °F) to 1755 °C (3191 °F)
SIGMA (N): liquid || 1255 °C (2291 °F) to 1755 °C (3191 °F)
return to listing
Ag - 45 Pd (wt %)
RHO (N): liquid || 1319 °C (2406 °F) to 1819 °C (3306 °F)
SIGMA (N): liquid || 1319 °C (2406 °F) to 1819 °C (3306 °F)
return to listing
Ag - 55 Pd (wt %)
RHO (N): liquid || 1373 °C (2503 °F) to 1873 °C (3403 °F)
SIGMA (N): liquid || 1373 °C (2503 °F) to 1873 °C (3403 °F)
return to listing
Ag - 65 Pd (wt %)
RHO (N): liquid || 1427 °C (2600 °F) to 1927 °C (3500 °F)
SIGMA (N): liquid || 1427 °C (2600 °F) to 1927 °C (3500 °F)
return to listing
Ag - 75 Pd (wt %)
RHO (N): liquid || 1464 °C (2667 °F) to 1964 °C (3567 °F)
SIGMA (N): liquid || 1464 °C (2667 °F) to 1964 °C (3567 °F)
return to listing
Ag - 85 Pd (wt %)
RHO (N): liquid || 1496 °C (2725 °F) to 1996 °C (3625 °F)
SIGMA (N): liquid || 1496 °C (2725 °F) to 1996 °C (3625 °F)
return to listing
Ag - 95 Pd (wt %)
RHO (N): liquid || 1532 °C (2789 °F) to 2032 °C (3689 °F)
SIGMA (N): liquid || 1532 °C (2789 °F) to 2032 °C (3689 °F)
return to listing
Ag - 99 Pd (wt %)
RHO (N): liquid || 1552 °C (2825 °F) to 2052 °C (3725 °F)
SIGMA (N): liquid || 1552 °C (2825 °F) to 2052 °C (3725 °F)
return to listing
Ag - 0.2 Zn (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -63 °C (-82 °F)
return to listing
Ag - 1 Zn (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -63 °C (-82 °F)
return to listing
Ag - 3.3 Zn (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -63 °C (-82 °F)
return to listing
Ag - 13 Zn (wt %) (New)
S : solid || alpha phase || -267.1 °C (-448.9 °F) to -63 °C (-82 °F)
return to listing
AgTl3Te2
D (N*): solid || monoclinic || room temperature value
return to listing
Al - 3 Li - 1.25 Mn (wt %) (11 a/o Li) (New)
UTS (*): extrusion || underaged, longitudinal || room temperature value
UTS (*): extrusion || underaged, long transverse || room temperature value
UTS (*): extrusion || peak aged, longitudinal || room temperature value
UTS (*): extrusion || peak aged, long transverse || room temperature value
YS (*): extrusion || underaged, longitudinal || room temperature value
YS (*): extrusion || underaged, long transverse || room temperature value
YS (*): extrusion || peak aged, longitudinal || room temperature value
YS (*): extrusion || peak aged, long transverse || room temperature value
%El (*): extrusion || underaged, longitudinal || room temperature value
%El (*): extrusion || underaged, long transverse || room temperature value
%El (*): extrusion || peak aged, longitudinal || room temperature value
%El (*): extrusion || peak aged, long transverse || room temperature value
FEN : extrusion || tested at 20 °C (68 °F), R = -1, axial, underaged, plastic strain amplitude || 9 cycles to 1.4 x 103 cycles
FEN : extrusion || tested at 20 °C (68 °F), R = -1, axial, peak aged, plastic strain amplitude || 4.7 cycles to 270 cycles
return to listing
Al - 2.5 Li (wt %) (9 a/o Li) (New)
DLL : solid || 20 °C (68 °F) to 567 °C (1052 °F)
MTE : solid || 20 °C (68 °F) to 567 °C (1052 °F)
CTE : solid || 20 °C (68 °F) to 567 °C (1052 °F)
D : solid || 20 °C (68 °F) to 567 °C (1052 °F)
E (*): extruded bar || underaged || room temperature value
UTS (*): extruded bar || underaged || room temperature value
UTS (*): extruded bar || peak aged || room temperature value
YS (*): extruded bar || underaged || room temperature value
YS (*): extruded bar || peak aged || room temperature value
%El (*): extruded bar || underaged || room temperature value
%El (*): extruded bar || peak aged || room temperature value
FEN : extruded bar, peak aged || tested at 20 °C (68 °F), R = -1, axial, plastic strain amplitude || 57 cycles to 2.1 x 103 cycles
return to listing
Al - 0.22 Mn (at %) (New)
S : solid || rapidly quenched || 20 °C (68 °F) to 170 °C (338 °F)
return to listing
Al - 0.5 Mn (at %) (New)
S : solid || rapidly quenched || -253.1 °C (-423.7 °F) to 165 °C (329 °F)
return to listing
Al - 2 Mn (at %) (New)
S : solid || rapidly quenched || -271.1 °C (-456.1 °F) to 70 °C (158 °F)
return to listing
Al - 6 Zn - 2 Mg - 0.5 Ni - 0.3 Fe (wt %)
D (N*): solid || room temperature value
return to listing
Al - 20 Zn (wt %) (New)
D (*): solid || room temperature value
UTS (*): as-cast || room temperature value
%El (*): as-cast || room temperature value
FSN : as-cast || tested at 20 °C (68 °F), R = -1, rotating beam, maximum stress || 3 x 104 cycles to 1 x 107 cycles
return to listing
AlB2
D (N*): solid || hexagonal, P6/mmm || room temperature value
return to listing
ALCHROME alloy D
UTS (N*): solid || room temperature value
YS (N*): solid || room temperature value
%El (N*): solid || room temperature value
return to listing
Al86Co14 (New)
RHO : solid || icosahedral symmetry || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
SIGMA : solid || icosahedral symmetry || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
alloy 90
DLL (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
MTE (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
CTE (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
D (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
SH (N*): solid || room temperature value
TD (N*): solid || annealed || room temperature value
TD (N*): solid || cold worked 10% || room temperature value
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
UTS (N*): annealed || room temperature value
UTS (N*): cold corked || room temperature value
%El (N*): solid || room temperature value
return to listing
alloy 30
DLL (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
MTE (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
CTE (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
D (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
TC (N*): solid || room temperature value
SH (N*): solid || room temperature value
TD (N*): solid || room temperature value
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
UTS (N*): annealed || room temperature value
UTS (N*): cold corked || room temperature value
%El (N*): solid || room temperature value
return to listing
Al3Ni2
D (N*): solid || trigonal, P-3m1 || room temperature value
return to listing
Al3Sc
RHO (N): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA (N): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
Arsenic
TC (N): solid || measured along the x-axis || -271.1 °C (-456.1 °F) to 27 °C (80 °F)
TD (N): solid || measured along the x-axis || 20 °C (68 °F) to 27 °C (80 °F)
RHO (N): solid || measured along the x-axis || -271.1 °C (-456.1 °F) to 32 °C (89 °F)
SIGMA (N): solid || measured along the x-axis || -271.1 °C (-456.1 °F) to 32 °C (89 °F)
S (N): solid || measured along the x-axis || -271.1 °C (-456.1 °F) to 27 °C (80 °F)
return to listing
Au - 30 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1200 °C (2192 °F)
return to listing
Au - 40 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1200 °C (2192 °F)
return to listing
Au - 50 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1200 °C (2192 °F)
return to listing
Au - 60 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1200 °C (2192 °F)
return to listing
Au - 70 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1200 °C (2192 °F)
return to listing
Au - 80 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1200 °C (2192 °F)
return to listing
Au - 90 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1200 °C (2192 °F)
return to listing
Au - 97 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1200 °C (2192 °F)
return to listing
Au - 99.5 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1200 °C (2192 °F)
return to listing
Au - 1 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 800 °C (1472 °F)
return to listing
Au - 2.2 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 800 °C (1472 °F)
return to listing
Au - 5 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 800 °C (1472 °F)
return to listing
Au - 15 Pd (wt %)
S (N): solid || -213.1 °C (-351.7 °F) to 1000 °C (1832 °F)
return to listing
AuCd
D (N*): solid || cubic, Pm-3m || room temperature value
D (N*): solid || orthorhombic, Pmma || room temperature value
D (N*): solid || trigonal, P31m || room temperature value
return to listing
AuPb2
D (N*): solid || tetragonal, I4/mcm || room temperature value
return to listing
AuSe
D (N*): solid || monoclinic || room temperature value
return to listing
AZ91
CRR (N): die cast || tested at 70 °C (158 °F) || 2 x 10-9/s to 1.2 x 10-3/s
CRR (N): die cast || tested at 135 °C (275 °F) || 1.8 x 10-8/s to 1.2 x 10-3/s
CRR (N): die cast || tested at 150 °C (302 °F) || 3.7 x 10-8/s to 1.3 x 10-6/s
CRR (N): die cast || tested at 180 °C (356 °F) || 1.4 x 10-8/s to 5 x 10-7/s
CRR (N): ingot || tested at 120 °C (248 °F) || 3.5 x 10-9/s to 4.7 x 10-8/s
CRR (N): ingot || tested at 150 °C (302 °F) || 6.1 x 10-8/s to 4 x 10-7/s
CRR (N): ingot || tested at 180 °C (356 °F) || 1.1 x 10-7/s to 1.3 x 10-6/s
CRR (N): thixoformed || tested at 120 °C (248 °F) || 6 x 10-10/s to 3.8 x 10-7/s
CRR (N): thixoformed || tested at 150 °C (302 °F) || 2.5 x 10-9/s to 1.3 x 10-6/s
CRR (N): thixoformed || tested at 180 °C (356 °F) || 1.2 x 10-9/s to 3 x 10-5/s
CRR (N): thixoformed, 4 h at 415 °C (779 °F) || tested at 120 °C (248 °F) || 5.7 x 10-11/s to 9.1 x 10-10/s
CRR (N): thixoformed, 4 h at 415 °C (779 °F) || tested at 150 °C (302 °F) || 1.1 x 10-9/s to 1.8 x 10-7/s
CRR (N): thixoformed, 4 h at 415 °C (779 °F) || tested at 180 °C (356 °F) || 2.7 x 10-9/s to 6 x 10-5/s
return to listing
BALCO alloy 400
DLL (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
MTE (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
CTE (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
D (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
return to listing
Ba2SiO4
D (N*): solid || orthorhombic || room temperature value
return to listing
BeSO4
D (N*): solid || tetragonal, I-4 || room temperature value
return to listing
Bi - 60 Rb (at %) Rb3Bi2 (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Bi - 58 Rb (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Bi - 53 Rb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 550 °C (1022 °F)
SIGMA : liquid || 450 °C (842 °F) to 550 °C (1022 °F)
return to listing
Bi - 48 Rb (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Bi - 90 Rb (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Bi2K3 (New)
RHO : liquid || 450 °C (842 °F) to 550 °C (1022 °F)
SIGMA : liquid || 450 °C (842 °F) to 550 °C (1022 °F)
return to listing
Bismuth
RHO (R): solid || polycrystal, annealed || -269.1 °C (-452.5 °F) to 247 °C (476 °F)
SIGMA (R): solid || polycrystal, annealed || -269.1 °C (-452.5 °F) to 247 °C (476 °F)
Vis (R): liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
return to listing
Ca - 40 Al - 10 Ga (at %) (New)
S : solid || glassy || -269.1 °C (-452.5 °F) to 10 °C (50 °F)
return to listing
Ca - 30 Al (at %) (New)
S : solid || glassy || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
Ca - 40 Al (at %) (New)
S : solid || glassy || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
Ca - 20 Al (at %) (New)
S : solid || glassy || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
CaAl4O7
D (N*): solid || monoclinic || room temperature value
return to listing
CaAl2Si2O8
D (N*): solid || triclinic || room temperature value
return to listing
2 CaCl2 - 4 MgCl2 - 4 NaCl - 90 H2O (wt %) (New)
TC : liquid || at 40 MPa (5.8 ksi) || 20 °C (68 °F) to 200 °C (392 °F)
TC : saturated liquid || 20 °C (68 °F) to 200 °C (392 °F)
return to listing
5 CaCl2 - 5 MgCl2 - 10 NaCl - 80 H2O (wt %) (New)
TC : liquid || at 40 MPa (5.8 ksi) || 20 °C (68 °F) to 200 °C (392 °F)
TC : saturated liquid || 20 °C (68 °F) to 200 °C (392 °F)
return to listing
3.33 CaCl2 - 6.67 NaCl - 90 H2O (wt %) (New)
TC : liquid || at 40 MPa (5.8 ksi) || 20 °C (68 °F) to 200 °C (392 °F)
TC : liquid || at 50 MPa (7.25 ksi) || 20 °C (68 °F) to 200 °C (392 °F)
TC : saturated liquid || 20 °C (68 °F) to 200 °C (392 °F)
return to listing
6.67 CaCl2 - 13.33 NaCl - 80 H2O (wt %) (New)
TC : liquid || at 40 MPa (5.8 ksi) || 20 °C (68 °F) to 200 °C (392 °F)
TC : liquid || at 50 MPa (7.25 ksi) || 20 °C (68 °F) to 200 °C (392 °F)
TC : saturated liquid || 20 °C (68 °F) to 200 °C (392 °F)
return to listing
CaC2O4
D (N*): solid || orthorhombic, Pbca || room temperature value
D (N*): solid || monoclinic, P2/m || room temperature value
return to listing
Cadmium
RHO (N): solid || polycrystal || -270.1 °C (-454.3 °F) to 54 °C (129 °F)
RHO (N): solid || a-axis || -270.1 °C (-454.3 °F) to 54 °C (129 °F)
RHO (N): solid || c-axis || -270.1 °C (-454.3 °F) to 54 °C (129 °F)
RHO (R): liquid || 320 °C (608 °F) to 645 °C (1193 °F)
SIGMA (N): solid || polycrystal || -270.1 °C (-454.3 °F) to 54 °C (129 °F)
SIGMA (N): solid || a-axis || -270.1 °C (-454.3 °F) to 54 °C (129 °F)
SIGMA (N): solid || c-axis || -270.1 °C (-454.3 °F) to 54 °C (129 °F)
SIGMA (R): liquid || 320 °C (608 °F) to 645 °C (1193 °F)
return to listing
CaF2
E (R): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
G (R): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
v (R): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
K (R): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
CaMoO4
D (N*): solid || tetragonal, I41/a || room temperature value
return to listing
Ca3SiO5
D (N*): solid || trigonal || room temperature value
return to listing
Ca3V2O8
D (N*): solid || trigonal || room temperature value
return to listing
Ca2V2O7
D (N*): solid || triclinic || room temperature value
return to listing
CaZn2Sb2
D (N*): solid || trigonal || room temperature value
return to listing
CBX Cupron
DLL (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
MTE (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
CTE (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
D (N): solid || 20 °C (68 °F) to 100 °C (212 °F)
UTS (N*): annealed || room temperature value
UTS (N*): cold corked || room temperature value
%El (N*): solid || room temperature value
return to listing
CdS
E (N*): solid || room temperature value
G (N*): solid || room temperature value
v (N*): solid || room temperature value
K (N*): solid || room temperature value
return to listing
CdSO4
D (N*): solid || orthorhombic, Pmn21 || room temperature value
D (N*): solid || orthorhombic, Cmnm || room temperature value
return to listing
CeAg (New)
RHO : solid || -257.1 °C (-430.9 °F) to 527 °C (980 °F)
SIGMA : solid || -257.1 °C (-430.9 °F) to 527 °C (980 °F)
return to listing
CeFe2 (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to 30 °C (86 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 30 °C (86 °F)
return to listing
CePd3 (New)
D (*): solid || room temperature value
SH : solid || -271.1 °C (-456.1 °F) to -259.1 °C (-434.5 °F)
HC : solid || -271.1 °C (-456.1 °F) to -259.1 °C (-434.5 °F)
RHO : solid || 24 Ce - 76 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || 24.8 Ce - 75.2 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || 25 Ce - 75 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || 25.3 Ce - 74.7 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || 25.7 Ce - 74.3 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || 26.5 Ce - 73.5 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || 24 Ce - 76 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || 24.8 Ce - 75.2 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || 25 Ce - 75 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || 25.3 Ce - 74.7 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || 25.7 Ce - 74.3 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || 26.5 Ce - 73.5 Pd (at %) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
C4F9OCH3 (Novec 71000) (New)
DLL : liquid || -135 °C (-211 °F) to 61 °C (142 °F)
MTE : liquid || -135 °C (-211 °F) to 61 °C (142 °F)
CTE : liquid || -135 °C (-211 °F) to 61 °C (142 °F)
D : liquid || -135 °C (-211 °F) to 61 °C (142 °F)
TC : vapor || 81 °C (178 °F) to 110 °C (230 °F)
VP : liquid || -135 °C (-211 °F) to 61 °C (142 °F)
return to listing
C7H8 - C10H16 mixtures (toluene/beta-pinene) (New)
SH : liquid || C7H8 || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 95 C7H8, 5 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 90 C7H8, 10 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 85 C7H8, 15 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 80 C7H8, 20 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 75 C7H8, 25 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 70 C7H8, 30 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 65 C7H8, 35 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 60 C7H8, 40 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 55 C7H8, 45 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 50 C7H8, 50 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 45 C7H8, 55 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 40 C7H8, 60 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 35 C7H8, 65 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 30 C7H8, 70 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 25 C7H8, 75 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 20 C7H8, 80 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 15 C7H8, 85 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 10 C7H8, 90 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 5 C7H8, 95 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || C10H16 || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || C7H8 || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 95 C7H8, 5 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 90 C7H8, 10 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 85 C7H8, 15 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 80 C7H8, 20 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 75 C7H8, 25 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 70 C7H8, 30 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 65 C7H8, 35 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 60 C7H8, 40 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 55 C7H8, 45 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 50 C7H8, 50 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 45 C7H8, 55 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 40 C7H8, 60 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 35 C7H8, 65 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 30 C7H8, 70 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 25 C7H8, 75 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 20 C7H8, 80 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 15 C7H8, 85 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 10 C7H8, 90 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 5 C7H8, 95 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || C10H16 || 20 °C (68 °F) to 75 °C (167 °F)
return to listing
C10H16 (alpha-pinene) (New)
D (*): liquid || room temperature value
SH : liquid || 20 °C (68 °F) to 100 °C (212 °F)
HC : liquid || 20 °C (68 °F) to 100 °C (212 °F)
Vis (*): liquid || room temperature value
ST (*): liquid || room temperature value
VP (*): liquid || room temperature value
return to listing
C2H6 (ethane)
ST (R): liquid || -140 °C (-220 °F) to 10 °C (50 °F)
return to listing
15 CH2F2 - 85 C2HF5 (wt %) (R-32/R-125) (New)
TC : vapor || at 100 kPa (14.5 psi) || 32 °C (89 °F) to 138 °C (280 °F)
TC : vapor || at 500 kPa (72.5 psi) || 32 °C (89 °F) to 138 °C (280 °F)
TC : vapor || at 1 MPa (145 psi) || 32 °C (89 °F) to 138 °C (280 °F)
TC : vapor || at 1.25 MPa (181 psi) || 32 °C (89 °F) to 138 °C (280 °F)
TC : vapor || at 1.5 MPa (218 psi) || 32 °C (89 °F) to 138 °C (280 °F)
TC : vapor || at 1.8 MPa (261 psi) || 32 °C (89 °F) to 138 °C (280 °F)
TC : saturated vapor || 32 °C (89 °F) to 138 °C (280 °F)
TC : ideal gas || at 100 kPa (14.5 psi), atmospheric pressure || 32 °C (89 °F) to 138 °C (280 °F)
return to listing
C3H2F6 (HFC-236ea)
D (N): saturated vapor || 20 °C (68 °F) to 139 °C (282 °F)
VP (N): saturated vapor || 20 °C (68 °F) to 139 °C (282 °F)
return to listing
C4H8O2 - C10H16 mixtures (ethyl acetate/beta-pinene) (New)
SH : liquid || C4H8O2 || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 95 C4H8O2, 5 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 90 C4H8O2, 10 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 85 C4H8O2, 15 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 80 C4H8O2, 20 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 75 C4H8O2, 25 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 70 C4H8O2, 30 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 65 C4H8O2, 35 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 60 C4H8O2, 40 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 55 C4H8O2, 45 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 50 C4H8O2, 50 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 45 C4H8O2, 55 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 40 C4H8O2, 60 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 35 C4H8O2, 65 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 30 C4H8O2, 70 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 25 C4H8O2, 75 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 20 C4H8O2, 80 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 15 C4H8O2, 85 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 10 C4H8O2, 90 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || 5 C4H8O2, 95 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
SH : liquid || C10H16 || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || C4H8O2 || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 95 C4H8O2, 5 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 90 C4H8O2, 10 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 85 C4H8O2, 15 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 80 C4H8O2, 20 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 75 C4H8O2, 25 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 70 C4H8O2, 30 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 65 C4H8O2, 35 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 60 C4H8O2, 40 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 55 C4H8O2, 45 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 50 C4H8O2, 50 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 45 C4H8O2, 55 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 40 C4H8O2, 60 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 35 C4H8O2, 65 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 30 C4H8O2, 70 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 25 C4H8O2, 75 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 20 C4H8O2, 80 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 15 C4H8O2, 85 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 10 C4H8O2, 90 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || 5 C4H8O2, 95 C10H16 (mol %) || 20 °C (68 °F) to 75 °C (167 °F)
HC : liquid || C10H16 || 20 °C (68 °F) to 75 °C (167 °F)
return to listing
Chromium
E (R): solid || -128 °C (-199 °F) to 1250 °C (2282 °F)
G (N): solid || -128 °C (-199 °F) to 55 °C (131 °F)
v (N): solid || -128 °C (-199 °F) to 55 °C (131 °F)
K (N): solid || -128 °C (-199 °F) to 55 °C (131 °F)
return to listing
C10M1 (R-21/R-22/R-142b) (New)
TC : liquid || at 1.75 MPa (254 psi) || 30 °C (86 °F) to 50 °C (122 °F)
TC : liquid || at 2.5 MPa (363 psi) || 30 °C (86 °F) to 70 °C (158 °F)
TC : liquid || at 3.4 MPa (493 psi) || 30 °C (86 °F) to 70 °C (158 °F)
TC : vapor || at 750 kPa (109 psi) || 50 °C (122 °F) to 125 °C (257 °F)
TC : vapor || at 1 MPa (145 psi) || 50 °C (122 °F) to 125 °C (257 °F)
TC : vapor || at 1.25 MPa (181 psi) || 65 °C (149 °F) to 125 °C (257 °F)
TC : vapor || at 1.5 MPa (218 psi) || 80 °C (176 °F) to 125 °C (257 °F)
TC : vapor || at 1.75 MPa (254 psi) || 80 °C (176 °F) to 125 °C (257 °F)
TC : vapor || at 2 MPa (290 psi) || 80 °C (176 °F) to 125 °C (257 °F)
return to listing
CoB
D (N*): solid || orthorhombic, Pnma || room temperature value
return to listing
Co0.6Ga0.4 (New)
RHO : solid || -173 °C (-280 °F) to 40 °C (104 °F)
SIGMA : solid || -173 °C (-280 °F) to 40 °C (104 °F)
return to listing
CoGa (New)
RHO : solid || -153 °C (-244 °F) to 47 °C (116 °F)
SIGMA : solid || -153 °C (-244 °F) to 47 °C (116 °F)
return to listing
Co2Ga1.95Cr0.05 (New)
RHO : solid || -263.1 °C (-441.7 °F) to 27 °C (80 °F)
SIGMA : solid || -263.1 °C (-441.7 °F) to 27 °C (80 °F)
return to listing
Co2Ga1.95Mn0.05 (New)
RHO : solid || -263.1 °C (-441.7 °F) to 27 °C (80 °F)
SIGMA : solid || -263.1 °C (-441.7 °F) to 27 °C (80 °F)
return to listing
Co80P20 (New)
RHO : solid || at 100 kPa (14.5 psi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || at 5.4 GPa (783 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || at 6.6 GPa (957 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || at 7 GPa (1.02 Msi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || at 9.5 GPa (1.38 Msi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 100 kPa (14.5 psi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 5.4 GPa (783 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 6.6 GPa (957 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 7 GPa (1.02 Msi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 9.5 GPa (1.38 Msi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
Co76P24 (New)
RHO : solid || amorphous || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || amorphous || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
Co3S4
D (N*): solid || cubic, Fd-3m || room temperature value
return to listing
Co3Se4
D (N*): solid || cubic, Fd-3m || room temperature value
D (N*): solid || monoclinic, C2/m || room temperature value
return to listing
CoSO4
D (N*): solid || orthorhombic, Cmcm || room temperature value
D (N*): solid || orthorhombic, Pnma || room temperature value
D (N*): solid || orthorhombic, P21/m || room temperature value
return to listing
Cr - 23.5 Fe (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Cr - 0.5 Ir (at %) (New)
D (*): solid || room temperature value
RHO : solid || -208.1 °C (-342.7 °F) to 250 °C (482 °F)
SIGMA : solid || -208.1 °C (-342.7 °F) to 250 °C (482 °F)
return to listing
Cr - 0.3 Mn (at %) (New)
D (*): solid || room temperature value
RHO : solid || -196.1 °C (-321.1 °F) to 150 °C (302 °F)
SIGMA : solid || -196.1 °C (-321.1 °F) to 150 °C (302 °F)
return to listing
Cr - 0.1 Mn (at %) (New)
D (*): solid || room temperature value
RHO : solid || -196.1 °C (-321.1 °F) to 175 °C (347 °F)
SIGMA : solid || -196.1 °C (-321.1 °F) to 175 °C (347 °F)
return to listing
0.5 Cr - 0.5 Mo - 0.25 V (wt %)
SR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 0.5 h at 950 °C (1742 °F), air cooled || 180 h to 2 x 104 h
SR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 0.5 h at 950 °C (1742 °F), oil quenched || 100 h to 4 x 104 h
SR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 0.5 h at 1050 °C (1922 °F), air cooled || 100 h to 5 x 104 h
SR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 0.5 h at 1050 °C (1922 °F), oil quenched || 155 h to 6 x 104 h
SR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 1 minute at 1300 °C (2372 °F), air cooled || 340 h to 3 x 104 h
SR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 1 minute at 1300 °C (2372 °F), oil quenched || 230 h to 3 x 104 h
CRR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 0.5 h at 950 °C (1742 °F), air cooled || 1.1 x 10-8/s to 6 x 10-6/s
CRR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 0.5 h at 1050 °C (1922 °F), air cooled || 1.1 x 10-8/s to 2 x 10-5/s
CRR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 1 minute at 1300 °C (2372 °F), air cooled || 1 x 10-8/s to 1.2 x 10-6/s
CRR (N): tempered at 700 °C (1292 °F) || tested at 550 °C (1022 °F), 2nd temper: 1 minute at 1300 °C (2372 °F), oil quenched || 3 x 10-9/s to 1.2 x 10-7/s
return to listing
Cr - 10.8 Mo (at %) (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
Cr - 21.2 Mo (at %) (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
Cr - 2 Mo (at %) (New)
D (*): solid || room temperature value
RHO : solid || -272.1 °C (-457.9 °F) to 45 °C (113 °F)
SIGMA : solid || -272.1 °C (-457.9 °F) to 45 °C (113 °F)
return to listing
CrAl7 (New)
RHO : solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
Cr11Ge19
D (N*): solid || tetragonal, P-4n2 || room temperature value
return to listing
Cr2N
D (N*): solid || trigonal, P-31m || room temperature value
return to listing
CrSb2
D (N*): solid || tetragonal, I4/mcm || room temperature value
D (N*): solid || orthorhombic, Pnnm || room temperature value
return to listing
Cr5Si3
RHO (N): solid || 205 nm thin film || -253.1 °C (-423.7 °F) to 830 °C (1526 °F)
SIGMA (N): solid || 205 nm thin film || -253.1 °C (-423.7 °F) to 830 °C (1526 °F)
return to listing
Cs - 50 Pb (at %)
RHO (N): liquid || 625 °C (1157 °F) to 725 °C (1337 °F)
SIGMA (N): liquid || 625 °C (1157 °F) to 725 °C (1337 °F)
return to listing
Cs - 60 Pb (at %)
RHO (N): liquid || 625 °C (1157 °F) to 725 °C (1337 °F)
SIGMA (N): liquid || 625 °C (1157 °F) to 725 °C (1337 °F)
return to listing
Cs - 70 Pb (at %)
RHO (N): liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA (N): liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Cs - 30 Pb (at %)
RHO (N): liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA (N): liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Cs - 45 Pb (at %)
RHO (N): liquid || 625 °C (1157 °F) to 725 °C (1337 °F)
SIGMA (N): liquid || 625 °C (1157 °F) to 725 °C (1337 °F)
return to listing
Cs - 25 Pb (at %) (New)
DLL : liquid || 483 °C (901 °F) to 752 °C (1385 °F)
MTE : liquid || 483 °C (901 °F) to 752 °C (1385 °F)
CTE : liquid || 483 °C (901 °F) to 752 °C (1385 °F)
D : liquid || 483 °C (901 °F) to 752 °C (1385 °F)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Cs - 35 Pb (at %) (New)
DLL : liquid || 508 °C (946 °F) to 752 °C (1385 °F)
MTE : liquid || 508 °C (946 °F) to 752 °C (1385 °F)
CTE : liquid || 508 °C (946 °F) to 752 °C (1385 °F)
D : liquid || 508 °C (946 °F) to 752 °C (1385 °F)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Cs - 5 Pb (at %) (New)
RHO : liquid || 425 °C (797 °F) to 525 °C (977 °F)
SIGMA : liquid || 425 °C (797 °F) to 525 °C (977 °F)
return to listing
Cs - 80 Pb (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Cs - 90 Pb (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
CsCaBi (New)
D (*): solid || room temperature value
return to listing
Cu - 4.5 Al (wt %)
E (N*): solid || room temperature value
G (N*): solid || room temperature value
v (N*): solid || room temperature value
K (N*): solid || room temperature value
return to listing
Cu - 0.5 Al (wt %)
E (N*): solid || room temperature value
G (N*): solid || room temperature value
v (N*): solid || room temperature value
K (N*): solid || room temperature value
return to listing
Cu - 3 Al (wt %)
E (N*): solid || room temperature value
G (N*): solid || room temperature value
v (N*): solid || room temperature value
K (N*): solid || room temperature value
return to listing
Cu - 50 Ni (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Cu - 1 Ni (wt %)
DLL (N): solid || 20 °C (68 °F) to 800 °C (1472 °F)
MTE (N): solid || 20 °C (68 °F) to 800 °C (1472 °F)
CTE (N): solid || 20 °C (68 °F) to 800 °C (1472 °F)
D (N): solid || 20 °C (68 °F) to 800 °C (1472 °F)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Cu - 5 Ni (wt %)
DLL (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
MTE (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
CTE (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
D (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Cu - 15 Ni (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Cu - 25 Ni (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Cu - 35 Ni (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
80 Cu - 14 Pb - 6 Fe (at %)
D (N*): solid || room temperature value
return to listing
80 Cu - 10 Pb - 10 Fe (at %)
D (N*): solid || room temperature value
return to listing
70 Cu - 24 Pb - 6 Fe (at %)
D (N*): solid || room temperature value
return to listing
90 Cu - 8 Pb - 2 Fe (at %)
D (N*): solid || room temperature value
return to listing
90 Cu - 4 Pb - 6 Fe (at %)
D (N*): solid || room temperature value
return to listing
80 Cu - 18 Pb - 2 Fe (at %)
D (N*): solid || room temperature value
return to listing
42 Cu - 58 Pb (at %)
D (N*): solid || room temperature value
return to listing
73 Cu - 27 Pb (wt %)
D (N*): solid || room temperature value
return to listing
75 Cu - 25 Pb (wt %) (New)
D (*): solid || room temperature value
E (*): as-cast || room temperature value
UTS (*): as-cast || room temperature value
YS (*): as-cast || room temperature value
%El (*): as-cast || room temperature value
FEN : as-cast || tested at 20 °C (68 °F), R = -1, axial, total strain amplitude || 50 cycles to 1.6 x 103 cycles
FEN : as-cast || tested at 20 °C (68 °F), R = -1, axial, plastic strain amplitude || 50 cycles to 1.6 x 103 cycles
FEN : as-cast || tested at 20 °C (68 °F), R = -1, axial, elastic strain amplitude || 50 cycles to 1.6 x 103 cycles
return to listing
CuAl
D (N*): solid || monoclinic, C2/m || room temperature value
return to listing
CuCr2O4
D (N*): solid || cubic || room temperature value
D (N*): solid || tetragonal || room temperature value
return to listing
Cu5FeS4
D (N*): solid || orthorhombic || room temperature value
return to listing
Cu1.8Mo6S8 (New)
SH : solid || -253.1 °C (-423.7 °F) to -210.1 °C (-346.3 °F)
HC : solid || -253.1 °C (-423.7 °F) to -210.1 °C (-346.3 °F)
S : solid || -263.1 °C (-441.7 °F) to 40 °C (104 °F)
return to listing
Cu1.8Mo6S5Se3 (New)
S : solid || -263.1 °C (-441.7 °F) to 20 °C (68 °F)
return to listing
Cu1.8Mo6S3Se5 (New)
S : solid || -263.1 °C (-441.7 °F) to 25 °C (77 °F)
return to listing
Cu1.8Mo6SSe7 (New)
SH : solid || -253.1 °C (-423.7 °F) to -210.1 °C (-346.3 °F)
HC : solid || -253.1 °C (-423.7 °F) to -210.1 °C (-346.3 °F)
S : solid || -263.1 °C (-441.7 °F) to 20 °C (68 °F)
return to listing
Cu1.8Mo6S6Se2 (New)
S : solid || -263.1 °C (-441.7 °F) to 40 °C (104 °F)
return to listing
Cu1.8Mo6S7Te (New)
S : solid || -263.1 °C (-441.7 °F) to 5 °C (41 °F)
return to listing
Cu1.8Mo6S5Te3 (New)
S : solid || -263.1 °C (-441.7 °F) to 20 °C (68 °F)
return to listing
Cu3Pd
D (N*): solid || cubic, Pm-3m || room temperature value
return to listing
Cu2Sb
D (N*): solid || tetragonal, P4/nmm || room temperature value
return to listing
CuSO4
D (N*): solid || orthorhombic, Pnma || room temperature value
return to listing
Cu66Ti34 (New)
RHO (*): solid || amorphous || room temperature value
SIGMA (*): solid || amorphous || room temperature value
return to listing
Cu45Zr55 (New)
RHO (*): solid || amorphous || room temperature value
SIGMA (*): solid || amorphous || room temperature value
S : solid || amorphous || -269.1 °C (-452.5 °F) to -50 °C (-58 °F)
return to listing
Cu60Zr40 (New)
RHO : solid || amorphous || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || amorphous || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
S : solid || amorphous || -269.1 °C (-452.5 °F) to -5 °C (23 °F)
return to listing
Cu50Zr40Fe10 (New)
S : solid || amorphous || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
return to listing
DP 1000
UTS (N*): 1.5 mm (0.0591 inch) sheet, parallel to the rolling direction || room temperature value
YS (N*): 1.5 mm (0.0591 inch) sheet, parallel to the rolling direction || room temperature value
return to listing
DyCo2
RHO (N): solid || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
SIGMA (N): solid || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
S (N): solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
DyS1.48 (New)
TC : solid || -193.1 °C (-315.7 °F) to 127 °C (260 °F)
return to listing
ErCo2 (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
S : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
EuP
D (N*): solid || cubic, Fm-3m || room temperature value
return to listing
Europium
RHO (N): solid || 20 °C (68 °F) to 827 °C (1520 °F)
RHO (N): liquid || 827 °C (1520 °F) to 912 °C (1673 °F)
SIGMA (N): solid || 20 °C (68 °F) to 827 °C (1520 °F)
SIGMA (N): liquid || 827 °C (1520 °F) to 912 °C (1673 °F)
S (N): solid || 20 °C (68 °F) to 827 °C (1520 °F)
S (N): liquid || 827 °C (1520 °F) to 912 °C (1673 °F)
return to listing
EuZn2Sb2
D (N*): solid || trigonal, P-3m1 || room temperature value
return to listing
Evanohm alloy S
TC (N*): solid || room temperature value
SH (N*): solid || room temperature value
TD (N*): solid || room temperature value
UTS (N*): 0.0254 mm (0.001 inch) diameter wire || room temperature value
UTS (N*): 0.0635 mm (0.0025 inch) diameter wire || room temperature value
UTS (N*): 0.16 mm (0.0063 inch) diameter wire || room temperature value
YS (N*): 0.0254 mm (0.001 inch) diameter wire || room temperature value
YS (N*): 0.0635 mm (0.0025 inch) diameter wire || room temperature value
YS (N*): 0.16 mm (0.0063 inch) diameter wire || room temperature value
%El (N*): 0.0254 mm (0.001 inch) diameter wire || room temperature value
%El (N*): 0.0635 mm (0.0025 inch) diameter wire || room temperature value
%El (N*): 0.16 mm (0.0063 inch) diameter wire || room temperature value
return to listing
Fe - 18 Cr - 2 Al - 1 Si - 1.25 Ta (wt %) (New)
D (*): solid || room temperature value
UTS (*): annealed, parallel to rolling direction || room temperature value
YS (*): annealed, parallel to rolling direction || room temperature value
%El (*): annealed, parallel to rolling direction || room temperature value
SR : annealed, parallel to rolling direction || tested at 800 °C (1472 °F) || 105 h to 2,800 h
SR : annealed, parallel to rolling direction || tested at 900 °C (1652 °F) || 130 h to 460 h
SR : annealed, parallel to rolling direction || tested at 1000 °C (1832 °F) || 7 h to 800 h
SR : annealed, parallel to rolling direction || Master curve (LMP) || 17.9 h to 22.2 h
return to listing
Fe - 15 Cr - 5 Al - 0.7 Y (wt %) (New)
D (*): solid || room temperature value
UTS (*): annealed, parallel to final rolling direction || room temperature value
YS (*): annealed, parallel to final rolling direction || room temperature value
%El (*): annealed, parallel to final rolling direction || room temperature value
SR : annealed, parallel to rolling direction || tested at 800 °C (1472 °F) || 0.7 h to 1,200 h
SR : annealed, parallel to rolling direction || tested at 900 °C (1652 °F) || 40 h to 500 h
SR : annealed, parallel to rolling direction || tested at 1000 °C (1832 °F) || 5 h to 4,200 h
SR : annealed, parallel to rolling direction || Master curve (LMP) || 11.2 h to 18 h
CRR : annealed, parallel to rolling direction || tested at 800 °C (1472 °F) || 3 x 10-8/s to 1.2 x 10-6/s
CRR : annealed, parallel to rolling direction || tested at 1000 °C (1832 °F) || 2 x 10-9/s to 3 x 10-6/s
CRR : annealed, perpendicular to rolling direction || tested at 1000 °C (1832 °F) || 3 x 10-10/s to 3 x 10-6/s
return to listing
Fe - 35 Ni - 25 Cr - 0.4 C (wt %) (various Nb additions) (New)
UTS (*): as-cast, 0.05 Nb (wt %) || room temperature value
UTS (*): as-cast, 0.89 Nb (wt %) || room temperature value
UTS (*): as-cast, 1.46 Nb (wt %) || room temperature value
UTS (*): as-cast, 2.56 Nb (wt %) || room temperature value
%El (*): as-cast, 0.05 Nb (wt %) || room temperature value
%El (*): as-cast, 0.89 Nb (wt %) || room temperature value
%El (*): as-cast, 1.46 Nb (wt %) || room temperature value
%El (*): as-cast, 2.56 Nb (wt %) || room temperature value
SR : as-cast, 0.05 Nb (wt %) || tested at 871 °C (1600 °F) || 18 h to 310 h
SR : as-cast, 0.05 Nb (wt %) || tested at 950 °C (1742 °F) || 3.1 h to 130 h
SR : as-cast, 0.05 Nb (wt %) || Master curve (LMP) || 30.1 h to 33.1 h
SR : as-cast, 0.42 Nb (wt %) || tested at 871 °C (1600 °F) || 30 h to 410 h
SR : as-cast, 0.42 Nb (wt %) || tested at 950 °C (1742 °F) || 2.8 h to 27 h
SR : as-cast, 0.42 Nb (wt %) || Master curve (LMP) || 28 h to 29.8 h
SR : as-cast, 0.89 Nb (wt %) || tested at 871 °C (1600 °F) || 60 h to 840 h
SR : as-cast, 0.89 Nb (wt %) || tested at 950 °C (1742 °F) || 9 h to 111 h
SR : as-cast, 0.89 Nb (wt %) || Master curve (LMP) || 23.8 h to 25.7 h
SR : as-cast, 1.46 Nb (wt %) || tested at 871 °C (1600 °F) || 110 h to 740 h
SR : as-cast, 1.46 Nb (wt %) || tested at 950 °C (1742 °F) || 10 h to 93 h
SR : as-cast, 1.46 Nb (wt %) || Master curve (LMP) || 22.4 h to 23.8 h
SR : as-cast, 2.56 Nb (wt %) || tested at 871 °C (1600 °F) || 55 h to 520 h
SR : as-cast, 2.56 Nb (wt %) || tested at 950 °C (1742 °F) || 8.3 h to 50 h
SR : as-cast, 2.56 Nb (wt %) || Master curve (LMP) || 22.6 h to 24 h
CRR : as-cast, 0.05 Nb (wt %) || tested at 871 °C (1600 °F) || 3 x 10-8/s to 5 x 10-7/s
CRR : as-cast, 0.05 Nb (wt %) || tested at 950 °C (1742 °F) || 3 x 10-8/s to 5 x 10-7/s
CRR : as-cast, 0.89 Nb (wt %) || tested at 871 °C (1600 °F) || 9 x 10-8/s to 2.7 x 10-7/s
CRR : as-cast, 0.89 Nb (wt %) || tested at 950 °C (1742 °F) || 5 x 10-8/s to 2.7 x 10-7/s
CRR : as-cast, 1.46 Nb (wt %) || tested at 871 °C (1600 °F) || 1.8 x 10-8/s to 1.3 x 10-7/s
CRR : as-cast, 1.46 Nb (wt %) || tested at 950 °C (1742 °F) || 3 x 10-8/s to 2 x 10-7/s
CRR : as-cast, 2.56 Nb (wt %) || tested at 871 °C (1600 °F) || 3 x 10-8/s to 1.4 x 10-7/s
CRR : as-cast, 2.56 Nb (wt %) || tested at 950 °C (1742 °F) || 4 x 10-8/s to 3 x 10-7/s
return to listing
50 Fe - 25 Ni - 25 Mn (wt %) (New)
D (*): solid || room temperature value
RHO : solid || -198.1 °C (-324.7 °F) to 997 °C (1826 °F)
SIGMA : solid || -198.1 °C (-324.7 °F) to 997 °C (1826 °F)
return to listing
51 Fe - 36 Ni - 13 Mn (wt %) (New)
D (*): solid || room temperature value
RHO : solid || -206.1 °C (-339.1 °F) to 987 °C (1808 °F)
SIGMA : solid || -206.1 °C (-339.1 °F) to 987 °C (1808 °F)
return to listing
50 Fe - 41 Ni - 9 Mn (wt %) (New)
D (*): solid || room temperature value
RHO : solid || -210.1 °C (-346.3 °F) to 1027 °C (1880 °F)
SIGMA : solid || -210.1 °C (-346.3 °F) to 1027 °C (1880 °F)
return to listing
47 Fe - 22 Ni - 31 Mn (wt %) (New)
D (*): solid || room temperature value
RHO : solid || -203.1 °C (-333.7 °F) to 1007 °C (1844 °F)
SIGMA : solid || -203.1 °C (-333.7 °F) to 1007 °C (1844 °F)
return to listing
Fe - 47 Rh - 3 Pd (at %) (New)
RHO : solid || -269.1 °C (-452.5 °F) to 600 °C (1112 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 600 °C (1112 °F)
return to listing
Fe - 49.8 Rh (at %) (New)
RHO : solid || -269.1 °C (-452.5 °F) to 490 °C (914 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 490 °C (914 °F)
return to listing
Fe - 50.2 Rh (at %) (New)
RHO : solid || -269.1 °C (-452.5 °F) to 500 °C (932 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 500 °C (932 °F)
return to listing
Fe - 48 Rh (at %) (New)
RHO : solid || -269.1 °C (-452.5 °F) to 490 °C (914 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 490 °C (914 °F)
return to listing
Fe - 4 Si (wt %)
CRR (N): in compression || tested at 1200 °C (2192 °F) || 7 x 10-7/s to 1.15 x 10-5/s
CRR (N): in compression || tested at 1250 °C (2282 °F) || 2 x 10-6/s to 2.7 x 10-5/s
CRR (N): in compression || tested at 1300 °C (2372 °F) || 5.5 x 10-6/s to 2.4 x 10-5/s
CRR (N): in compression || tested at 1350 °C (2462 °F) || 3.5 x 10-6/s to 2.7 x 10-5/s
CRR (N): in compression || tested at 1400 °C (2552 °F) || 4.7 x 10-6/s to 1.25 x 10-5/s
return to listing
FeB
D (N*): solid || orthorhombic, Cmcm || room temperature value
D (N*): solid || orthorhombic, Pnma || room temperature value
D (N*): solid || tetragonal, I41/amd || room temperature value
return to listing
FeCo (New)
D (*): solid || room temperature value
RHO : solid || quenched from 815 °C (1499 °F) || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
RHO : solid || quenched from 739 °C (1362 °F) || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
RHO : solid || quenched from 720 °C (1328 °F) || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
RHO : solid || quenched from 700 °C (1292 °F) || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
RHO : solid || quenched from 680 °C (1256 °F) || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
RHO : solid || quenched from 620 °C (1148 °F) || -269.1 °C (-452.5 °F) to -5 °C (23 °F)
RHO : solid || furnace cooled || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || quenched from 815 °C (1499 °F) || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
SIGMA : solid || quenched from 739 °C (1362 °F) || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || quenched from 720 °C (1328 °F) || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || quenched from 700 °C (1292 °F) || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
SIGMA : solid || quenched from 680 °C (1256 °F) || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
SIGMA : solid || quenched from 620 °C (1148 °F) || -269.1 °C (-452.5 °F) to -5 °C (23 °F)
SIGMA : solid || furnace cooled || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
Fe0.643Cr0.201Ni0.156 (New)
D (*): solid || room temperature value
SH : solid || -38 °C (-37 °F) to 927 °C (1700 °F)
HC : solid || -38 °C (-37 °F) to 927 °C (1700 °F)
return to listing
Fe0.472Cr0.197Ni0.331 (New)
D (*): solid || room temperature value
SH : solid || -8 °C (17 °F) to 927 °C (1700 °F)
HC : solid || -8 °C (17 °F) to 927 °C (1700 °F)
return to listing
Fe0.691Cr0.194Ni0.115 (New)
D (*): solid || room temperature value
SH : solid || -33 °C (-28 °F) to 927 °C (1700 °F)
HC : solid || -33 °C (-28 °F) to 927 °C (1700 °F)
return to listing
Fe1.4Mn1.6Si (New)
SH : solid || -263.1 °C (-441.7 °F) to 0 °C (32 °F)
HC : solid || -263.1 °C (-441.7 °F) to 0 °C (32 °F)
return to listing
Fe2.2Mn0.8Si (New)
SH : solid || -263.1 °C (-441.7 °F) to 140 °C (284 °F)
HC : solid || -263.1 °C (-441.7 °F) to 140 °C (284 °F)
return to listing
Fe2N
D (N*): solid || orthorhombic, Pbcn || room temperature value
D (N*): solid || trigonal, P-31m || room temperature value
return to listing
Fe32Ni36Cr14P12B6 (New)
RHO : solid || amorphous || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
RHO : solid || crystallized || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || amorphous || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || crystallized || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
(Fe1-xNix)90Zr10 (New)
RHO : solid || Fe90Zr10 || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || (Fe0.9Ni0.1)90Zr10 || -269.1 °C (-452.5 °F) to 370 °C (698 °F)
RHO : solid || (Fe0.8Ni0.2)90Zr10 || -269.1 °C (-452.5 °F) to 370 °C (698 °F)
RHO : solid || (Fe0.75Ni0.25)90Zr10 || -269.1 °C (-452.5 °F) to 355 °C (671 °F)
RHO : solid || (Fe0.7Ni0.3)90Zr10 || -269.1 °C (-452.5 °F) to 370 °C (698 °F)
RHO : solid || (Fe0.6Ni0.4)90Zr10 || -269.1 °C (-452.5 °F) to 355 °C (671 °F)
SIGMA : solid || Fe90Zr10 || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || (Fe0.9Ni0.1)90Zr10 || -269.1 °C (-452.5 °F) to 370 °C (698 °F)
SIGMA : solid || (Fe0.8Ni0.2)90Zr10 || -269.1 °C (-452.5 °F) to 370 °C (698 °F)
SIGMA : solid || (Fe0.75Ni0.25)90Zr10 || -269.1 °C (-452.5 °F) to 355 °C (671 °F)
SIGMA : solid || (Fe0.7Ni0.3)90Zr10 || -269.1 °C (-452.5 °F) to 370 °C (698 °F)
SIGMA : solid || (Fe0.6Ni0.4)90Zr10 || -269.1 °C (-452.5 °F) to 355 °C (671 °F)
return to listing
FeSb2
D (N*): solid || tetragonal, I4/mcm || room temperature value
D (N*): solid || orthorhombic, Pnnm || room temperature value
return to listing
FeSi2
D (N*): solid || tetragonal, P4/mmm || room temperature value
return to listing
Fe2(SO4)3
D (N*): solid || monoclinic, P21/c || room temperature value
D (N*): solid || trigonal, R-3 || room temperature value
return to listing
FeTe2
D (N*): solid || orthorhombic, Pnnm || room temperature value
return to listing
Fe2TiSn
D (N*): solid || cubic || room temperature value
return to listing
Fe2V1-xAl1+x
D (N*): solid || cubic, Fm-3m || room temperature value
return to listing
GaAs
E (N): solid || polycrystal || -273.1 °C (-459.7 °F) to 1240 °C (2264 °F)
G (N): solid || polycrystal || -273.1 °C (-459.7 °F) to 1240 °C (2264 °F)
v (N): solid || polycrystal || -273.1 °C (-459.7 °F) to 1240 °C (2264 °F)
K (N): solid || polycrystal || -273.1 °C (-459.7 °F) to 1240 °C (2264 °F)
return to listing
GaFeO3 (Sm doped)
D (N*): solid || orthorhombic, Pna21 || room temperature value
return to listing
Gallium
DLL (N): solid || polycrystal || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
DLL (N): solid || a-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
DLL (N): solid || b-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
DLL (N): solid || c-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
MTE (N): solid || polycrystal || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
MTE (N): solid || a-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
MTE (N): solid || b-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
MTE (N): solid || c-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
CTE (N): solid || polycrystal || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
CTE (N): solid || a-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
CTE (N): solid || b-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
CTE (N): solid || c-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
D (N): solid || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
RHO (R): solid || polycrystal || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
RHO (R): solid || a-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
RHO (R): solid || b-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
RHO (R): solid || c-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
RHO (R): liquid || 0 °C (32 °F) to 752 °C (1385 °F)
SIGMA (R): solid || polycrystal || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
SIGMA (R): solid || a-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
SIGMA (R): solid || b-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
SIGMA (R): solid || c-axis || -183.1 °C (-297.7 °F) to 30 °C (86 °F)
SIGMA (R): liquid || 0 °C (32 °F) to 752 °C (1385 °F)
return to listing
Ga2Se3
D (N*): solid || monoclinic, Cc || room temperature value
return to listing
Gd - 40 Y (at %) (New)
D (*): solid || room temperature value
E (*): solid || polycrystal || room temperature value
E (*): solid || a-axis || room temperature value
E (*): solid || c-axis || room temperature value
return to listing
Gd4Co3 (New)
SH : solid || -269.1 °C (-452.5 °F) to 23 °C (73 °F)
HC : solid || -269.1 °C (-452.5 °F) to 23 °C (73 °F)
RHO : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
S : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
Gd3Ga5O12 (Cr, Eu, Nd, Sm, & Tb doped)
DLL (R): solid || 20 °C (68 °F) to 1227 °C (2240 °F)
MTE (R): solid || 20 °C (68 °F) to 1227 °C (2240 °F)
CTE (R): solid || 20 °C (68 °F) to 1227 °C (2240 °F)
D (R): solid || 20 °C (68 °F) to 1227 °C (2240 °F)
return to listing
GdNi (New)
SH : solid || -271.1 °C (-456.1 °F) to -183.1 °C (-297.7 °F)
HC : solid || -271.1 °C (-456.1 °F) to -183.1 °C (-297.7 °F)
return to listing
GdP
D (N*): solid || cubic, Fm-3m || room temperature value
return to listing
Gd3Sc2Ga3O12
DLL (N): solid || Gd3.04Sc1.8Ga3.16O12 || 20 °C (68 °F) to 1227 °C (2240 °F)
MTE (N): solid || Gd3.04Sc1.8Ga3.16O12 || 20 °C (68 °F) to 1227 °C (2240 °F)
CTE (N): solid || Gd3.04Sc1.8Ga3.16O12 || 20 °C (68 °F) to 1227 °C (2240 °F)
D (N): solid || Gd3.04Sc1.8Ga3.16O12 || 20 °C (68 °F) to 1227 °C (2240 °F)
return to listing
(Gd0.4Y0.6)4Co3 (New)
RHO : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
S : solid || -269.1 °C (-452.5 °F) to 10 °C (50 °F)
return to listing
(Gd0.2Y0.8)4Co3 (New)
RHO : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
S : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
(Gd0.9Y0.1)4Co3 (New)
RHO : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
(Gd0.7Y0.3)4Co3 (New)
RHO : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
GeSe2
D (N*): solid || tetragonal, I-42d || room temperature value
D (N*): solid || orthorhombic, Fdd2 || room temperature value
D (N*): solid || monoclinic, P21/c || room temperature value
return to listing
Graphite AXF-5Q
DLL (N): solid || bulk density = 1.78 g/cm3 || 20 °C (68 °F) to 1327 °C (2420 °F)
MTE (N): solid || bulk density = 1.78 g/cm3 || 20 °C (68 °F) to 1327 °C (2420 °F)
CTE (N): solid || bulk density = 1.78 g/cm3 || 20 °C (68 °F) to 1327 °C (2420 °F)
D (N): solid || bulk density = 1.78 g/cm3 || 20 °C (68 °F) to 1327 °C (2420 °F)
return to listing
Hafnium
E (N): solid || -269.1 °C (-452.5 °F) to 25 °C (77 °F)
G (N): solid || -269.1 °C (-452.5 °F) to 25 °C (77 °F)
v (N): solid || -269.1 °C (-452.5 °F) to 25 °C (77 °F)
K (N): solid || -269.1 °C (-452.5 °F) to 25 °C (77 °F)
return to listing
HfNiSn
D (N*): solid || cubic, F-43m || room temperature value
return to listing
Hf0.5Zr0.5V2 (New)
E : solid || -263.1 °C (-441.7 °F) to 20 °C (68 °F)
return to listing
Hf0.75Zr0.25V2 (New)
E : solid || -253.1 °C (-423.7 °F) to 20 °C (68 °F)
return to listing
Hg - 10 Cs (at %) (New)
RHO : liquid || 137 °C (278 °F) to 340 °C (644 °F)
SIGMA : liquid || 137 °C (278 °F) to 340 °C (644 °F)
S : liquid || 137 °C (278 °F) to 350 °C (662 °F)
return to listing
Hg - 2 Cs (at %) (New)
RHO : liquid || -43 °C (-46 °F) to 340 °C (644 °F)
SIGMA : liquid || -43 °C (-46 °F) to 340 °C (644 °F)
S : liquid || -43 °C (-46 °F) to 350 °C (662 °F)
return to listing
Hg - 6 Cs (at %) (New)
RHO : liquid || 14 °C (57 °F) to 340 °C (644 °F)
SIGMA : liquid || 14 °C (57 °F) to 340 °C (644 °F)
S : liquid || 14 °C (57 °F) to 350 °C (662 °F)
return to listing
Hg - 8 K (at %) (New)
RHO : liquid || 72 °C (161 °F) to 250 °C (482 °F)
SIGMA : liquid || 72 °C (161 °F) to 250 °C (482 °F)
S : liquid || 72 °C (161 °F) to 360 °C (680 °F)
return to listing
Hg - 2 K (at %) (New)
RHO : liquid || 17 °C (62 °F) to 250 °C (482 °F)
SIGMA : liquid || 17 °C (62 °F) to 250 °C (482 °F)
S : liquid || 17 °C (62 °F) to 360 °C (680 °F)
return to listing
Hg - 6 K (at %) (New)
RHO : liquid || 61 °C (142 °F) to 250 °C (482 °F)
SIGMA : liquid || 61 °C (142 °F) to 250 °C (482 °F)
S : liquid || 61 °C (142 °F) to 360 °C (680 °F)
return to listing
Hg - 4 Li (at %) (New)
RHO : liquid || 100 °C (212 °F) to 240 °C (464 °F)
SIGMA : liquid || 100 °C (212 °F) to 240 °C (464 °F)
S : liquid || 200 °C (392 °F) to 240 °C (464 °F)
return to listing
Hg - 6 Li (at %) (New)
RHO : liquid || 100 °C (212 °F) to 240 °C (464 °F)
SIGMA : liquid || 100 °C (212 °F) to 240 °C (464 °F)
S : liquid || 200 °C (392 °F) to 240 °C (464 °F)
return to listing
Hg - 4 Na (at %) (New)
DLL : liquid || -15 °C (5 °F) to 250 °C (482 °F)
MTE : liquid || -15 °C (5 °F) to 250 °C (482 °F)
CTE : liquid || -15 °C (5 °F) to 250 °C (482 °F)
D : liquid || -15 °C (5 °F) to 250 °C (482 °F)
return to listing
Hg - 6 Na (at %) (New)
DLL : liquid || 29 °C (84 °F) to 250 °C (482 °F)
MTE : liquid || 29 °C (84 °F) to 250 °C (482 °F)
CTE : liquid || 29 °C (84 °F) to 250 °C (482 °F)
D : liquid || 29 °C (84 °F) to 250 °C (482 °F)
return to listing
Hg - 10 Na (at %) (New)
DLL : liquid || 89 °C (192 °F) to 250 °C (482 °F)
MTE : liquid || 89 °C (192 °F) to 250 °C (482 °F)
CTE : liquid || 89 °C (192 °F) to 250 °C (482 °F)
D : liquid || 89 °C (192 °F) to 250 °C (482 °F)
return to listing
Hg - 14 Na (at %) (New)
DLL : liquid || 130 °C (266 °F) to 250 °C (482 °F)
MTE : liquid || 130 °C (266 °F) to 250 °C (482 °F)
CTE : liquid || 130 °C (266 °F) to 250 °C (482 °F)
D : liquid || 130 °C (266 °F) to 250 °C (482 °F)
return to listing
Hg - 8 Tl (at %) (New)
RHO : liquid || -58 °C (-73 °F) to 340 °C (644 °F)
SIGMA : liquid || -58 °C (-73 °F) to 340 °C (644 °F)
S : liquid || -58 °C (-73 °F) to 327 °C (620 °F)
return to listing
Hg - 12 Tl (at %) (New)
RHO : liquid || -36 °C (-33 °F) to 340 °C (644 °F)
SIGMA : liquid || -36 °C (-33 °F) to 340 °C (644 °F)
S : liquid || -36 °C (-33 °F) to 327 °C (620 °F)
return to listing
Hg - 4 Tl (at %) (New)
RHO : liquid || -47 °C (-53 °F) to 340 °C (644 °F)
SIGMA : liquid || -47 °C (-53 °F) to 340 °C (644 °F)
S : liquid || -47 °C (-53 °F) to 327 °C (620 °F)
return to listing
HgCr2Se4
DLL (R): solid || 20 °C (68 °F) to 497 °C (926 °F)
MTE (R): solid || 20 °C (68 °F) to 497 °C (926 °F)
CTE (R): solid || 20 °C (68 °F) to 497 °C (926 °F)
D (N): solid || 20 °C (68 °F) to 497 °C (926 °F)
return to listing
HoCo2 (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to -10 °C (14 °F)
S : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
HoZn (New)
D (*): solid || room temperature value
SH : solid || -253.1 °C (-423.7 °F) to 25 °C (77 °F)
HC : solid || -253.1 °C (-423.7 °F) to 25 °C (77 °F)
return to listing
HY-80
UTS (N*): quenched from 900 °C (1652 °F), tempered 590 °C (1094 °F) || room temperature value
YS (N*): quenched from 900 °C (1652 °F), tempered 590 °C (1094 °F) || room temperature value
%El (N*): quenched from 900 °C (1652 °F), tempered 590 °C (1094 °F) || room temperature value
return to listing
InAs
E (N): solid || polycrystal || -273.1 °C (-459.7 °F) to 27 °C (80 °F)
G (N): solid || polycrystal || -248.1 °C (-414.7 °F) to 27 °C (80 °F)
v (N): solid || polycrystal || -248.1 °C (-414.7 °F) to 27 °C (80 °F)
K (N): solid || polycrystal || -248.1 °C (-414.7 °F) to 27 °C (80 °F)
return to listing
Inconel 600
SSCC (N): 0.001/s, Srinivasan & Prasad || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, Srinivasan & Prasad || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, Srinivasan & Prasad || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, Srinivasan & Prasad || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, Srinivasan & Prasad || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, Srinivasan & Prasad || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, Srinivasan & Prasad || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, Srinivasan & Prasad || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, Srinivasan & Prasad || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, Srinivasan & Prasad || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, Srinivasan & Prasad || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, Srinivasan & Prasad || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, Srinivasan & Prasad || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, Srinivasan & Prasad || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, Srinivasan & Prasad || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, Srinivasan & Prasad || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, Srinivasan & Prasad || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, Srinivasan & Prasad || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, Srinivasan & Prasad || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, Srinivasan & Prasad || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, Srinivasan & Prasad || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, Srinivasan & Prasad || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, Srinivasan & Prasad || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, Srinivasan & Prasad || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, Srinivasan & Prasad || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, Srinivasan & Prasad || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, Srinivasan & Prasad || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, Srinivasan & Prasad || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, Srinivasan & Prasad || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, Srinivasan & Prasad || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, Srinivasan & Prasad || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, Srinivasan & Prasad || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, Srinivasan & Prasad || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, Srinivasan & Prasad || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, Srinivasan & Prasad || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, Srinivasan & Prasad || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, Srinivasan & Prasad || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, Srinivasan & Prasad || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, Srinivasan & Prasad || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, Srinivasan & Prasad || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, Srinivasan & Prasad || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, Srinivasan & Prasad || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, Srinivasan & Prasad || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, Srinivasan & Prasad || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, Srinivasan & Prasad || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, Srinivasan & Prasad || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, Srinivasan & Prasad || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, Srinivasan & Prasad || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
return to listing
Inconel C-276
DLL (R): solid || 20 °C (68 °F) to 871 °C (1600 °F)
MTE (R): solid || 20 °C (68 °F) to 871 °C (1600 °F)
CTE (R): solid || 20 °C (68 °F) to 871 °C (1600 °F)
D (R): solid || 20 °C (68 °F) to 871 °C (1600 °F)
return to listing
InS
D (N*): solid || monoclinic, P21/c || room temperature value
D (N*): solid || orthorhombic, Pnnm || room temperature value
return to listing
In2(SO4)3
D (N*): solid || trigonal, R-3 || room temperature value
D (N*): solid || monoclinic, P21/c || room temperature value
return to listing
Iron
CRR (N): in compression || tested at 1100 °C (2012 °F) || 1.05 x 10-6/s to 1 x 10-5/s
CRR (N): in compression || tested at 1200 °C (2192 °F) || 8 x 10-7/s to 9 x 10-6/s
CRR (N): in compression || tested at 1300 °C (2372 °F) || 1 x 10-6/s to 1 x 10-5/s
return to listing
K - 59 In (at %) (New)
RHO : liquid || 475 °C (887 °F) to 525 °C (977 °F)
SIGMA : liquid || 475 °C (887 °F) to 525 °C (977 °F)
return to listing
K - 20 In (at %) (New)
RHO : liquid || 475 °C (887 °F) to 525 °C (977 °F)
SIGMA : liquid || 475 °C (887 °F) to 525 °C (977 °F)
return to listing
K - 40 In (at %) (New)
RHO : liquid || 475 °C (887 °F) to 525 °C (977 °F)
SIGMA : liquid || 475 °C (887 °F) to 525 °C (977 °F)
return to listing
K - 47 In (at %) (New)
RHO : liquid || 475 °C (887 °F) to 525 °C (977 °F)
SIGMA : liquid || 475 °C (887 °F) to 525 °C (977 °F)
return to listing
K - 53 In (at %) (New)
RHO : liquid || 475 °C (887 °F) to 525 °C (977 °F)
SIGMA : liquid || 475 °C (887 °F) to 525 °C (977 °F)
return to listing
K - 50 Pb (at %) (KPb)
RHO (N): liquid || 575 °C (1067 °F) to 625 °C (1157 °F)
SIGMA (N): liquid || 575 °C (1067 °F) to 625 °C (1157 °F)
return to listing
K - 30 Pb (at %)
RHO (N): liquid || 400 °C (752 °F) to 575 °C (1067 °F)
SIGMA (N): liquid || 400 °C (752 °F) to 575 °C (1067 °F)
return to listing
K - 45 Pb (at %) (New)
RHO : liquid || 575 °C (1067 °F) to 625 °C (1157 °F)
SIGMA : liquid || 575 °C (1067 °F) to 625 °C (1157 °F)
return to listing
K - 60 Pb (at %) (New)
RHO : liquid || 575 °C (1067 °F) to 625 °C (1157 °F)
SIGMA : liquid || 575 °C (1067 °F) to 625 °C (1157 °F)
return to listing
KAlSi3O8
D (N*): solid || triclinic || room temperature value
return to listing
Kanthal Cuprothal 15
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Kanthal Manganina 43
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
28.9 KF - 71.1 LiF (mol %) (New)
DLL : liquid || 682 °C (1259 °F) to 917 °C (1682 °F)
MTE : liquid || 682 °C (1259 °F) to 917 °C (1682 °F)
CTE : liquid || 682 °C (1259 °F) to 917 °C (1682 °F)
D : liquid || 682 °C (1259 °F) to 917 °C (1682 °F)
return to listing
16Kh12V2FTaR (New)
DLL : solid || martensite || 20 °C (68 °F) to 600 °C (1112 °F)
DLL : solid || ferrite and perlite || 20 °C (68 °F) to 600 °C (1112 °F)
MTE : solid || martensite || 20 °C (68 °F) to 600 °C (1112 °F)
MTE : solid || ferrite and perlite || 20 °C (68 °F) to 600 °C (1112 °F)
CTE : solid || martensite || 20 °C (68 °F) to 600 °C (1112 °F)
CTE : solid || ferrite and perlite || 20 °C (68 °F) to 600 °C (1112 °F)
D : solid || martensite || 20 °C (68 °F) to 600 °C (1112 °F)
D : solid || ferrite and perlite || 20 °C (68 °F) to 600 °C (1112 °F)
return to listing
KPb
RHO (N): liquid || 575 °C (1067 °F) to 625 °C (1157 °F)
SIGMA (N): liquid || 575 °C (1067 °F) to 625 °C (1157 °F)
return to listing
K2SiO3
D (N*): solid || monoclinic || room temperature value
return to listing
316L
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 600 °C (1112 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 650 °C (1202 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 700 °C (1292 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 750 °C (1382 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 800 °C (1472 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.001/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1250 °C (2282 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 600 °C (1112 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 650 °C (1202 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 700 °C (1292 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 750 °C (1382 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 800 °C (1472 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.01/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1250 °C (2282 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 600 °C (1112 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 650 °C (1202 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 700 °C (1292 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 750 °C (1382 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 800 °C (1472 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 0.1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1250 °C (2282 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 600 °C (1112 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 650 °C (1202 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 700 °C (1292 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 750 °C (1382 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 800 °C (1472 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 1/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1250 °C (2282 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 600 °C (1112 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 650 °C (1202 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 700 °C (1292 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 750 °C (1382 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 800 °C (1472 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 10/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1250 °C (2282 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 600 °C (1112 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 650 °C (1202 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 700 °C (1292 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 750 °C (1382 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 800 °C (1472 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 850 °C (1562 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 900 °C (1652 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 950 °C (1742 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1000 °C (1832 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1050 °C (1922 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1100 °C (2012 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1150 °C (2102 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1200 °C (2192 °F) || 0.1 to 0.5 mm/mm strain
SSCC (N): 100/s, cold swagged bar, annealed at 1050 °C (1922 °F), Venugopal et al. || tested at 1250 °C (2282 °F) || 0.1 to 0.5 mm/mm strain
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched || tested at 350 °C (662 °F), R = -1, axial, total strain amplitude || 3 x 103 cycles to 1.7 x 104 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched || tested at 350 °C (662 °F), R = -1, axial, plastic strain amplitude || 3 x 103 cycles to 1.7 x 104 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched || tested at 350 °C (662 °F), R = -1, axial, elastic strain amplitude || 3 x 103 cycles to 1.7 x 104 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched || tested at 450 °C (842 °F), R = -1, axial, total strain amplitude || 2.3 x 103 cycles to 9.9 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched || tested at 450 °C (842 °F), R = -1, axial, plastic strain amplitude || 2.3 x 103 cycles to 9.9 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched || tested at 450 °C (842 °F), R = -1, axial, elastic strain amplitude || 2.3 x 103 cycles to 9.9 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched || tested at 550 °C (1022 °F), R = -1, axial, total strain amplitude || 680 cycles to 6 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched || tested at 550 °C (1022 °F), R = -1, axial, plastic strain amplitude || 680 cycles to 6 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched || tested at 550 °C (1022 °F), R = -1, axial, elastic strain amplitude || 680 cycles to 6 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched, aged 15 minutes at 750 °C (1382 °F) || tested at 350 °C (662 °F), R = -1, axial, total strain amplitude || 4.1 x 103 cycles to 3.9 x 104 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched, aged 15 minutes at 750 °C (1382 °F) || tested at 350 °C (662 °F), R = -1, axial, plastic strain amplitude || 4.1 x 103 cycles to 3.9 x 104 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched, aged 15 minutes at 750 °C (1382 °F) || tested at 350 °C (662 °F), R = -1, axial, elastic strain amplitude || 4.1 x 103 cycles to 3.9 x 104 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched, aged 15 minutes at 750 °C (1382 °F) || tested at 450 °C (842 °F), R = -1, axial, total strain amplitude || 1.9 x 103 cycles to 6.4 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched, aged 15 minutes at 750 °C (1382 °F) || tested at 450 °C (842 °F), R = -1, axial, plastic strain amplitude || 1.9 x 103 cycles to 6.4 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched, aged 15 minutes at 750 °C (1382 °F) || tested at 450 °C (842 °F), R = -1, axial, elastic strain amplitude || 1.9 x 103 cycles to 6.4 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched, aged 15 minutes at 750 °C (1382 °F) || tested at 550 °C (1022 °F), R = -1, axial, total strain amplitude || 350 cycles to 4.9 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched, aged 15 minutes at 750 °C (1382 °F) || tested at 550 °C (1022 °F), R = -1, axial, plastic strain amplitude || 350 cycles to 4.9 x 103 cycles
FEN (N): solution annealed at 1080 °C (1976 °F), water quenched, aged 15 minutes at 750 °C (1382 °F) || tested at 550 °C (1022 °F), R = -1, axial, elastic strain amplitude || 350 cycles to 4.9 x 103 cycles
CRR (N): submerged-arc butt welds || tested at 600 °C (1112 °F) || 2 x 10-9/s to 9.9 x 10-8/s
return to listing
La - 20 Al (at %) (New)
S : solid || amorphous || -269.1 °C (-452.5 °F) to 10 °C (50 °F)
return to listing
La - 28 Al (at %) (New)
S : solid || amorphous || -269.1 °C (-452.5 °F) to 10 °C (50 °F)
return to listing
LaCrO3 (Ca & Sr doped)
D (N*): solid || undoped, trigonal || room temperature value
D (N*): solid || undoped, orthorhombic || room temperature value
D (N*): solid || undoped, cubic || room temperature value
return to listing
Lanthanum
DLL (N): solid || 1.2 Fe (at %) || 20 °C (68 °F) to 889 °C (1632 °F)
DLL (R): liquid || 1.2 Fe (at %) || 889 °C (1632 °F) to 1427 °C (2600 °F)
MTE (N): solid || 1.2 Fe (at %) || 20 °C (68 °F) to 889 °C (1632 °F)
MTE (R): liquid || 1.2 Fe (at %) || 889 °C (1632 °F) to 1427 °C (2600 °F)
CTE (N): solid || 1.2 Fe (at %) || 20 °C (68 °F) to 889 °C (1632 °F)
CTE (R): liquid || 1.2 Fe (at %) || 889 °C (1632 °F) to 1427 °C (2600 °F)
D (N): solid || 1.2 Fe (at %) || 20 °C (68 °F) to 889 °C (1632 °F)
D (R): liquid || 1.2 Fe (at %) || 889 °C (1632 °F) to 1427 °C (2600 °F)
TC (N): solid || 1.2 Fe (at %) || 20 °C (68 °F) to 889 °C (1632 °F)
TC (R): liquid || 889 °C (1632 °F) to 1727 °C (3140 °F)
SH (N): solid || 1.2 Fe (at %) || 20 °C (68 °F) to 889 °C (1632 °F)
HC (N): solid || 1.2 Fe (at %) || 20 °C (68 °F) to 889 °C (1632 °F)
TD (N): solid || 1.2 Fe (at %) || 20 °C (68 °F) to 889 °C (1632 °F)
TD (R): liquid || 1.2 Fe (at %) || 889 °C (1632 °F) to 1427 °C (2600 °F)
RHO (R): liquid || 1027 °C (1880 °F) to 1727 °C (3140 °F)
SIGMA (R): liquid || 1027 °C (1880 °F) to 1727 °C (3140 °F)
return to listing
LaPO4
D (N*): solid || hexagonal, P622-2 || room temperature value
D (N*): solid || monoclinic, P21/c || room temperature value
return to listing
Lead
TC (R): liquid || 327 °C (620 °F) to 1000 °C (1832 °F)
TD (R): liquid || 328 °C (622 °F) to 1000 °C (1832 °F)
RHO (R): liquid || 232 °C (449 °F) to 800 °C (1472 °F)
SIGMA (R): liquid || 232 °C (449 °F) to 800 °C (1472 °F)
Vis (R): liquid || 328 °C (622 °F) to 1100 °C (2012 °F)
E (R): solid || -273.1 °C (-459.7 °F) to 150 °C (302 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 150 °C (302 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 150 °C (302 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 150 °C (302 °F)
return to listing
Li - 25 Cd (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Li - 35 Cd (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Li - 45 Cd (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Li - 55 Cd (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Li - 65 Cd (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Li - 75 Cd (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Li - 85 Cd (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Li - 95 Cd (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Li - 10 Cd (at %) (New)
RHO : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
SIGMA : liquid || 550 °C (1022 °F) to 650 °C (1202 °F)
return to listing
Li - 80 Ga (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 90 Ga (at %) (New)
RHO : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
SIGMA : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
return to listing
Li - 5 Ga (at %) (New)
RHO : liquid || 300 °C (572 °F) to 400 °C (752 °F)
SIGMA : liquid || 300 °C (572 °F) to 400 °C (752 °F)
return to listing
Li - 15 Ga (at %) (New)
RHO : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
SIGMA : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
return to listing
Li - 25 Ga (at %) (New)
RHO : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
SIGMA : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
return to listing
Li - 32 Ga (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 40 Ga (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 50 Ga (at %) (New)
RHO : liquid || 775 °C (1427 °F) to 875 °C (1607 °F)
SIGMA : liquid || 775 °C (1427 °F) to 875 °C (1607 °F)
return to listing
Li - 60 Ga (at %) (New)
RHO : liquid || 775 °C (1427 °F) to 875 °C (1607 °F)
SIGMA : liquid || 775 °C (1427 °F) to 875 °C (1607 °F)
return to listing
Li - 70 Ga (at %) (New)
RHO : liquid || 775 °C (1427 °F) to 875 °C (1607 °F)
SIGMA : liquid || 775 °C (1427 °F) to 875 °C (1607 °F)
return to listing
Li - 80 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 90 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 5 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 15 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 25 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 30 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 40 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 50 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 60 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
Li - 70 In (at %) (New)
RHO : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
SIGMA : liquid || 650 °C (1202 °F) to 750 °C (1382 °F)
return to listing
80 Li - 20 Pb (at %) (Li4Pb)
SH (N): liquid || 712 °C (1313 °F) to 987 °C (1808 °F)
HC (N): liquid || 712 °C (1313 °F) to 987 °C (1808 °F)
RHO (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
SIGMA (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
return to listing
75 Li - 25 Pb (at %) (Li3Pb)
SH (N): liquid || 697 °C (1286 °F) to 984 °C (1803 °F)
HC (N): liquid || 697 °C (1286 °F) to 984 °C (1803 °F)
RHO (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
SIGMA (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
return to listing
85 Li - 15 Pb (at %)
SH (N): liquid || 617 °C (1142 °F) to 925 °C (1697 °F)
RHO (N): liquid || 600 °C (1112 °F) to 726 °C (1339 °F)
SIGMA (N): liquid || 600 °C (1112 °F) to 726 °C (1339 °F)
return to listing
70 Li - 30 Pb (at %)
SH (N): liquid || 637 °C (1178 °F) to 984 °C (1803 °F)
RHO (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
SIGMA (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
return to listing
90 Li - 10 Pb (at %)
SH (N): liquid || 550 °C (1022 °F) to 907 °C (1664 °F)
return to listing
30 Li - 70 Pb (at %)
SH (N): liquid || 353 °C (667 °F) to 982 °C (1799 °F)
return to listing
14.2 Li - 85.8 Pb (at %) (New)
DLL : liquid || 244 °C (471 °F) to 728 °C (1342 °F)
MTE : liquid || 244 °C (471 °F) to 728 °C (1342 °F)
CTE : liquid || 244 °C (471 °F) to 728 °C (1342 °F)
D : liquid || 244 °C (471 °F) to 728 °C (1342 °F)
SH : liquid || 285 °C (545 °F) to 527 °C (980 °F)
ST : liquid || 360 °C (680 °F) to 435 °C (815 °F)
return to listing
10 Li - 90 Pb (at %) (New)
DLL : liquid || 273 °C (523 °F) to 728 °C (1342 °F)
MTE : liquid || 273 °C (523 °F) to 728 °C (1342 °F)
CTE : liquid || 273 °C (523 °F) to 728 °C (1342 °F)
D : liquid || 273 °C (523 °F) to 728 °C (1342 °F)
SH : liquid || 285 °C (545 °F) to 967 °C (1772 °F)
ST : liquid || 360 °C (680 °F) to 435 °C (815 °F)
return to listing
5.3 Li - 94.7 Pb (at %) (New)
DLL : liquid || 301 °C (574 °F) to 728 °C (1342 °F)
MTE : liquid || 301 °C (574 °F) to 728 °C (1342 °F)
CTE : liquid || 301 °C (574 °F) to 728 °C (1342 °F)
D : liquid || 301 °C (574 °F) to 728 °C (1342 °F)
SH : liquid || 328 °C (622 °F) to 967 °C (1772 °F)
ST : liquid || 360 °C (680 °F) to 435 °C (815 °F)
return to listing
2.7 Li - 97.3 Pb (at %) (New)
DLL : liquid || 314 °C (597 °F) to 728 °C (1342 °F)
MTE : liquid || 314 °C (597 °F) to 728 °C (1342 °F)
CTE : liquid || 314 °C (597 °F) to 728 °C (1342 °F)
D : liquid || 314 °C (597 °F) to 728 °C (1342 °F)
SH : liquid || 328 °C (622 °F) to 967 °C (1772 °F)
ST : liquid || 360 °C (680 °F) to 435 °C (815 °F)
return to listing
45 Li - 55 Pb (at %) (New)
SH : liquid || 462 °C (863 °F) to 990 °C (1814 °F)
return to listing
55 Li - 45 Pb (at %) (New)
DLL : liquid || 477 °C (890 °F) to 719 °C (1326 °F)
MTE : liquid || 477 °C (890 °F) to 719 °C (1326 °F)
CTE : liquid || 477 °C (890 °F) to 719 °C (1326 °F)
D : liquid || 477 °C (890 °F) to 719 °C (1326 °F)
RHO : liquid || 400 °C (752 °F) to 600 °C (1112 °F)
SIGMA : liquid || 400 °C (752 °F) to 600 °C (1112 °F)
return to listing
20 Li - 80 Pb (at %) (New)
DLL : liquid || 262 °C (503 °F) to 977 °C (1790 °F)
MTE : liquid || 262 °C (503 °F) to 977 °C (1790 °F)
CTE : liquid || 262 °C (503 °F) to 977 °C (1790 °F)
D : liquid || 262 °C (503 °F) to 977 °C (1790 °F)
SH : liquid || 309 °C (588 °F) to 527 °C (980 °F)
ST : liquid || 270 °C (518 °F) to 430 °C (806 °F)
return to listing
18 Li - 82 Pb (at %) (New)
DLL : liquid || 257 °C (494 °F) to 728 °C (1342 °F)
MTE : liquid || 257 °C (494 °F) to 728 °C (1342 °F)
CTE : liquid || 257 °C (494 °F) to 728 °C (1342 °F)
D : liquid || 257 °C (494 °F) to 728 °C (1342 °F)
SH : liquid || 309 °C (588 °F) to 527 °C (980 °F)
ST : liquid || 360 °C (680 °F) to 435 °C (815 °F)
return to listing
60 Li - 40 Sn (at %) (New)
RHO : solid || 542 °C (1007 °F) to 602 °C (1115 °F)
SIGMA : solid || 542 °C (1007 °F) to 602 °C (1115 °F)
return to listing
50 Li - 50 Sn (at %) (New)
RHO : solid || 498 °C (928 °F) to 558 °C (1036 °F)
SIGMA : solid || 498 °C (928 °F) to 558 °C (1036 °F)
return to listing
40 Li - 60 Sn (at %) (New)
RHO : solid || 453 °C (847 °F) to 513 °C (955 °F)
SIGMA : solid || 453 °C (847 °F) to 513 °C (955 °F)
return to listing
30 Li - 70 Sn (at %) (New)
RHO : solid || 380 °C (716 °F) to 440 °C (824 °F)
SIGMA : solid || 380 °C (716 °F) to 440 °C (824 °F)
return to listing
20 Li - 80 Sn (at %) (New)
RHO : solid || 323 °C (613 °F) to 383 °C (721 °F)
SIGMA : solid || 323 °C (613 °F) to 383 °C (721 °F)
return to listing
10 Li - 90 Sn (at %) (New)
RHO : solid || 270 °C (518 °F) to 330 °C (626 °F)
SIGMA : solid || 270 °C (518 °F) to 330 °C (626 °F)
return to listing
80 Li - 20 Sn (at %) (New)
RHO : solid || 780 °C (1436 °F) to 840 °C (1544 °F)
SIGMA : solid || 780 °C (1436 °F) to 840 °C (1544 °F)
return to listing
70 Li - 30 Sn (at %) (New)
RHO : solid || 725 °C (1337 °F) to 785 °C (1445 °F)
SIGMA : solid || 725 °C (1337 °F) to 785 °C (1445 °F)
return to listing
LiAlSi2O6
D (N*): solid || monoclinic || room temperature value
D (N*): solid || triclinic || room temperature value
return to listing
Li2B4O7
D (N*): solid || tetragonal, I41cd || room temperature value
return to listing
LiFeO2
D (N*): solid || trigonal || room temperature value
return to listing
Li3Pb
SH (N): liquid || 697 °C (1286 °F) to 984 °C (1803 °F)
HC (N): liquid || 697 °C (1286 °F) to 984 °C (1803 °F)
RHO (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
SIGMA (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
return to listing
Li4Pb
SH (N): liquid || 712 °C (1313 °F) to 987 °C (1808 °F)
HC (N): liquid || 712 °C (1313 °F) to 987 °C (1808 °F)
RHO (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
SIGMA (N): liquid || 726 °C (1339 °F) to 800 °C (1472 °F)
return to listing
Li4P2O7
D (N*): solid || triclinic, P-1 || room temperature value
D (N*): solid || monoclinic, P21/c || room temperature value
return to listing
Lithium
E (R): solid || -195.1 °C (-319.3 °F) to 25 °C (77 °F)
G (R): solid || -195.1 °C (-319.3 °F) to 25 °C (77 °F)
v (R): solid || -195.1 °C (-319.3 °F) to 25 °C (77 °F)
K (R): solid || -195.1 °C (-319.3 °F) to 25 °C (77 °F)
return to listing
LuFeO3
D (N*): solid || hexagonal || room temperature value
return to listing
300M
UTS (N): austenitized at 900 °C (1652 °F) || transformed at 320 °C (608 °F), oil quenched, tempered at 200 °C (392 °F) || -90 °C (-130 °F) to 20 °C (68 °F)
UTS (N): austenitized at 900 °C (1652 °F) || transformed at 350 °C (662 °F), oil quenched, tempered at 200 °C (392 °F) || -90 °C (-130 °F) to 20 °C (68 °F)
UTS (N): austenitized at 900 °C (1652 °F) || oil quenched, tempered at 200 °C (392 °F) || -90 °C (-130 °F) to 20 °C (68 °F)
YS (N): austenitized at 900 °C (1652 °F) || transformed at 320 °C (608 °F), oil quenched, tempered at 200 °C (392 °F) || -90 °C (-130 °F) to 20 °C (68 °F)
YS (N): austenitized at 900 °C (1652 °F) || transformed at 350 °C (662 °F), oil quenched, tempered at 200 °C (392 °F) || -90 °C (-130 °F) to 20 °C (68 °F)
YS (N): austenitized at 900 °C (1652 °F) || oil quenched, tempered at 200 °C (392 °F) || -90 °C (-130 °F) to 20 °C (68 °F)
%El (N): austenitized at 900 °C (1652 °F) || transformed at 320 °C (608 °F), oil quenched, tempered at 200 °C (392 °F) || -90 °C (-130 °F) to 20 °C (68 °F)
%El (N): austenitized at 900 °C (1652 °F) || transformed at 350 °C (662 °F), oil quenched, tempered at 200 °C (392 °F) || -90 °C (-130 °F) to 20 °C (68 °F)
%El (N): austenitized at 900 °C (1652 °F) || oil quenched, tempered at 200 °C (392 °F) || -90 °C (-130 °F) to 20 °C (68 °F)
return to listing
Manganin alloy 130
UTS (N*): annealed || room temperature value
UTS (N*): cold corked || room temperature value
return to listing
Mercury
S (N): liquid || 200 °C (392 °F) to 240 °C (464 °F)
return to listing
Mg - 4 Li - 5 Al (wt %)
DLL (N): solid || 20 °C (68 °F) to 350 °C (662 °F)
MTE (N): solid || 20 °C (68 °F) to 350 °C (662 °F)
CTE (N): solid || 20 °C (68 °F) to 350 °C (662 °F)
TC (N): solid || 20 °C (68 °F) to 200 °C (392 °F)
TD (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Mg - 21 Li (at %)
D (N*): solid || room temperature value
return to listing
Mg - 30 Li (at %)
DLL (N): solid || 20 °C (68 °F) to 504 °C (939 °F)
MTE (N): solid || 20 °C (68 °F) to 504 °C (939 °F)
CTE (N): solid || 20 °C (68 °F) to 504 °C (939 °F)
D (N): solid || 20 °C (68 °F) to 504 °C (939 °F)
TC (N): solid || 20 °C (68 °F) to 504 °C (939 °F)
TD (N): solid || 20 °C (68 °F) to 504 °C (939 °F)
return to listing
Mg - 32 Li (at %) (New)
DLL : solid || 20 °C (68 °F) to 376 °C (709 °F)
MTE : solid || 20 °C (68 °F) to 376 °C (709 °F)
CTE : solid || 20 °C (68 °F) to 376 °C (709 °F)
D : solid || 20 °C (68 °F) to 376 °C (709 °F)
TC : solid || 20 °C (68 °F) to 300 °C (572 °F)
SH : solid || 20 °C (68 °F) to 300 °C (572 °F)
TD : solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Mg - 1 Si (wt %)
SSC (N): 0.8 wt% Si || tested at 20 °C (68 °F), as-cast, unknown strain rate || 0 to 0.87 mm/mm strain
SSC (N): 0.8 wt% Si || tested at 20 °C (68 °F), hot-rolled at 15/s, unknown strain rate || 0 to 0.66 mm/mm strain
SSC (N): 0.8 wt% Si || tested at 20 °C (68 °F), hot-rolled at 20/s, unknown strain rate || 0 to 0.69 mm/mm strain
SSC (N): 0.8 wt% Si || tested at 20 °C (68 °F), hot-rolled at 25/s, unknown strain rate || 0 to 0.66 mm/mm strain
return to listing
Mg - 25 Zn (at %) (New)
S (*): solid || amorphous || room temperature value
return to listing
Mg - 33 Zn (at %) (New)
S (*): solid || amorphous || room temperature value
return to listing
MgAgSb
D (N*): solid || tetragonal, P4/nmm || room temperature value
D (N*): solid || cubic || room temperature value
return to listing
Mg3Au
D (N*): solid || hexagonal, P63/mmc || room temperature value
return to listing
MgB4
D (N*): solid || orthorhombic, Pnma || room temperature value
return to listing
Mg2C3
D (N*): solid || orthorhombic || room temperature value
return to listing
Mg(OH)2
D (N*): solid || monoclinic, P-3m1 || room temperature value
D (N*): solid || monoclinic, C2 || room temperature value
return to listing
MnAl6 (New)
D (*): solid || orthorhombic, Cmcm || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
Mn2B
D (N*): solid || tetragonal, I4/mcm || room temperature value
return to listing
Mn23C6
D (N*): solid || cubic, Fm-3m || room temperature value
D (N*): solid || monoclinic, C2/c || room temperature value
return to listing
Mn7C3
D (N*): solid || orthorhombic, Pnma || room temperature value
return to listing
Mn3CuN
D (N): solid || antiperovskite || -267.1 °C (-448.9 °F) to 127 °C (260 °F)
return to listing
Mn3P
D (N*): solid || tetragonal, I-4 || room temperature value
return to listing
Mn2P
D (N*): solid || hexagonal, P-62m || room temperature value
return to listing
MnSe
D (N*): solid || hexagonal, P63mc || room temperature value
D (N*): solid || cubic, F-43m || room temperature value
D (N*): solid || cubic, Fm-3m || room temperature value
return to listing
Mn3Si
D (N*): solid || cubic, Fm-3m || room temperature value
return to listing
MnSO4
D (N*): solid || orthorhombic, Cmcm || room temperature value
return to listing
MnWO4
D (N*): solid || monoclinic, P2/c || room temperature value
return to listing
Molybdenum
E (R): solid || polycrystal || -269.1 °C (-452.5 °F) to 1930 °C (3506 °F)
G (R): solid || polycrystal || -269.1 °C (-452.5 °F) to 1930 °C (3506 °F)
v (R): solid || polycrystal || -269.1 °C (-452.5 °F) to 1930 °C (3506 °F)
K (R): solid || polycrystal || -269.1 °C (-452.5 °F) to 1840 °C (3344 °F)
return to listing
Mo2S3
D (N*): solid || monoclinic, P21/m || room temperature value
return to listing
Mo3Si
D (N*): solid || cubic, Pm-3n || room temperature value
return to listing
Mo3Te4
D (N*): solid || trigonal, R-3 || room temperature value
return to listing
50 Na - 50 Bi (at %) (NaBi) (New)
RHO : liquid || 600 °C (1112 °F) to 850 °C (1562 °F)
SIGMA : liquid || 600 °C (1112 °F) to 850 °C (1562 °F)
return to listing
73 Na - 27 Bi (at %) (New)
RHO : liquid || 800 °C (1472 °F) to 850 °C (1562 °F)
SIGMA : liquid || 800 °C (1472 °F) to 850 °C (1562 °F)
return to listing
64 Na - 36 Bi (at %) (New)
RHO : liquid || 800 °C (1472 °F) to 850 °C (1562 °F)
SIGMA : liquid || 800 °C (1472 °F) to 850 °C (1562 °F)
return to listing
55 Na - 45 Bi (at %) (New)
RHO : liquid || 600 °C (1112 °F) to 850 °C (1562 °F)
SIGMA : liquid || 600 °C (1112 °F) to 850 °C (1562 °F)
return to listing
40 Na - 60 Bi (at %) (New)
RHO : liquid || 600 °C (1112 °F) to 850 °C (1562 °F)
SIGMA : liquid || 600 °C (1112 °F) to 850 °C (1562 °F)
return to listing
20 Na - 80 Bi (at %) (New)
RHO : liquid || 350 °C (662 °F) to 600 °C (1112 °F)
SIGMA : liquid || 350 °C (662 °F) to 600 °C (1112 °F)
return to listing
5 Na - 95 Bi (at %) (New)
RHO : liquid || 350 °C (662 °F) to 600 °C (1112 °F)
SIGMA : liquid || 350 °C (662 °F) to 600 °C (1112 °F)
return to listing
Na - 2.5 Pb (at %)
RHO (N): liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA (N): liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 7.5 Pb (at %)
RHO (N): liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA (N): liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 22.5 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 30 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 40 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 50 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 60 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 70 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 80 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 90 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 15 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na - 20 Pb (at %) (New)
RHO : liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA : liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
57 Na - 43 Sn (at %) (Na4Sn3) (New)
RHO : solid || 489 °C (912 °F) to 549 °C (1020 °F)
SIGMA : solid || 489 °C (912 °F) to 549 °C (1020 °F)
return to listing
70 Na - 30 Sn (at %) (New)
RHO : solid || 485 °C (905 °F) to 545 °C (1013 °F)
SIGMA : solid || 485 °C (905 °F) to 545 °C (1013 °F)
return to listing
60 Na - 40 Sn (at %) (New)
RHO : solid || 475 °C (887 °F) to 535 °C (995 °F)
SIGMA : solid || 475 °C (887 °F) to 535 °C (995 °F)
return to listing
55 Na - 45 Sn (at %) (New)
RHO : solid || 540 °C (1004 °F) to 600 °C (1112 °F)
SIGMA : solid || 540 °C (1004 °F) to 600 °C (1112 °F)
return to listing
45 Na - 55 Sn (at %) (New)
RHO : solid || 570 °C (1058 °F) to 630 °C (1166 °F)
SIGMA : solid || 570 °C (1058 °F) to 630 °C (1166 °F)
return to listing
35 Na - 65 Sn (at %) (New)
RHO : solid || 457 °C (854 °F) to 517 °C (962 °F)
SIGMA : solid || 457 °C (854 °F) to 517 °C (962 °F)
return to listing
25 Na - 75 Sn (at %) (New)
RHO : solid || 360 °C (680 °F) to 420 °C (788 °F)
SIGMA : solid || 360 °C (680 °F) to 420 °C (788 °F)
return to listing
15 Na - 85 Sn (at %) (New)
RHO : solid || 300 °C (572 °F) to 360 °C (680 °F)
SIGMA : solid || 300 °C (572 °F) to 360 °C (680 °F)
return to listing
5 Na - 95 Sn (at %) (New)
RHO : solid || 232 °C (449 °F) to 292 °C (557 °F)
SIGMA : solid || 232 °C (449 °F) to 292 °C (557 °F)
return to listing
85 Na - 15 Sn (at %) (New)
RHO : solid || 398 °C (748 °F) to 458 °C (856 °F)
SIGMA : solid || 398 °C (748 °F) to 458 °C (856 °F)
return to listing
77 Na - 23 Sn (at %) (New)
RHO : solid || 435 °C (815 °F) to 495 °C (923 °F)
SIGMA : solid || 435 °C (815 °F) to 495 °C (923 °F)
return to listing
NaAlSi2O6
D (N*): solid || monoclinic || room temperature value
return to listing
NaAlSiO4
D (N*): solid || cubic || room temperature value
D (N*): solid || hexagonal || room temperature value
return to listing
NaBi (New)
RHO : liquid || 600 °C (1112 °F) to 850 °C (1562 °F)
SIGMA : liquid || 600 °C (1112 °F) to 850 °C (1562 °F)
return to listing
NaB3O5
D (N*): solid || monoclinic, P21/c || room temperature value
return to listing
NaCl
E (R): solid || -269.1 °C (-452.5 °F) to 800 °C (1472 °F)
G (R): solid || -269.1 °C (-452.5 °F) to 800 °C (1472 °F)
v (R): solid || -269.1 °C (-452.5 °F) to 800 °C (1472 °F)
K (R): solid || -269.1 °C (-452.5 °F) to 800 °C (1472 °F)
return to listing
NaF
E (N): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
G (N): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
v (N): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
K (N): solid || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
NaFeO2
D (N*): solid || tetragonal || room temperature value
D (N*): solid || orthorhombic || room temperature value
return to listing
NaHCO3
D (N*): solid || monoclinic, P21/c || room temperature value
return to listing
Na15Pb4
TC (N): liquid || 350 °C (662 °F) to 800 °C (1472 °F)
SH (N): liquid || 372 °C (701 °F) to 800 °C (1472 °F)
HC (N): liquid || 372 °C (701 °F) to 800 °C (1472 °F)
TD (N): liquid || 387 °C (728 °F) to 677 °C (1250 °F)
RHO (N): liquid || 450 °C (842 °F) to 500 °C (932 °F)
SIGMA (N): liquid || 450 °C (842 °F) to 500 °C (932 °F)
return to listing
Na2Si2O5
D (N*): solid || tetragonal || room temperature value
D (N*): solid || orthorhombic || room temperature value
D (N*): solid || monoclinic || room temperature value
return to listing
Na2Ti3O7
D (N*): solid || monoclinic || room temperature value
return to listing
Nb - 5 Mo (wt %)
E (N): solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
G (N): solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
v (N): solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
K (N): solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
return to listing
Nb - 16 Mo (wt %) (New)
D (*): solid || room temperature value
E : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
G : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
v : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
K : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
return to listing
Nb - 34 Mo (wt %) (New)
D (*): solid || room temperature value
E : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
G : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
v : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
K : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
return to listing
Nb - 43 Mo (wt %) (New)
D (*): solid || room temperature value
E : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
G : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
v : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
K : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
return to listing
Nb - 57 Mo (wt %) (New)
D (*): solid || room temperature value
E : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
G : solid || polycrystal || -269.1 °C (-452.5 °F) to 2090 °C (3794 °F)
v : solid || polycrystal || -269.1 °C (-452.5 °F) to 2090 °C (3794 °F)
K : solid || polycrystal || -269.1 °C (-452.5 °F) to 2090 °C (3794 °F)
return to listing
Nb - 67 Mo (wt %) (New)
D (*): solid || room temperature value
E : solid || polycrystal || -269.1 °C (-452.5 °F) to 2085 °C (3785 °F)
G : solid || polycrystal || -269.1 °C (-452.5 °F) to 2085 °C (3785 °F)
v : solid || polycrystal || -269.1 °C (-452.5 °F) to 2085 °C (3785 °F)
K : solid || polycrystal || -269.1 °C (-452.5 °F) to 2085 °C (3785 °F)
return to listing
Nb - 75 Mo (wt %) (New)
D (*): solid || room temperature value
E : solid || polycrystal || -269.1 °C (-452.5 °F) to 1885 °C (3425 °F)
G : solid || polycrystal || -269.1 °C (-452.5 °F) to 1885 °C (3425 °F)
v : solid || polycrystal || -269.1 °C (-452.5 °F) to 1885 °C (3425 °F)
K : solid || polycrystal || -269.1 °C (-452.5 °F) to 1885 °C (3425 °F)
return to listing
Nb - 88 Mo (wt %) (New)
D (*): solid || room temperature value
E : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
G : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
v : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
K : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
return to listing
Nb - 7 Mo (wt %) (New)
D (*): solid || room temperature value
E : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
G : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
v : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
K : solid || polycrystal || -269.1 °C (-452.5 °F) to 1935 °C (3515 °F)
return to listing
Nb - 5 V (wt %) (B-33)
E (N*): solid || room temperature value
G (N*): solid || room temperature value
v (N*): solid || room temperature value
K (N*): solid || room temperature value
return to listing
Nb - 90 V (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Nb - 20 V (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Nb - 40 V (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Nb - 60 V (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Nb - 25 Zr (wt %)
RHO (N): solid, Morton et al. || as-rolled || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
RHO (N): solid, Morton et al. || annealed at 1500 °C (2732 °F) and quenched || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
RHO (N): solid, Morton et al. || quenched from 1500 °C (2732 °F), aged 10 minutes at 800 °C (1472 °F) || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
RHO (N): solid, Morton et al. || quenched from 1500 °C (2732 °F), aged 1 h at 800 °C (1472 °F) || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
RHO (N): solid, Morton et al. || quenched from 1500 °C (2732 °F), aged 5 h at 800 °C (1472 °F) || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
SIGMA (N): solid, Morton et al. || as-rolled || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
SIGMA (N): solid, Morton et al. || annealed at 1500 °C (2732 °F) and quenched || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
SIGMA (N): solid, Morton et al. || quenched from 1500 °C (2732 °F), aged 10 minutes at 800 °C (1472 °F) || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
SIGMA (N): solid, Morton et al. || quenched from 1500 °C (2732 °F), aged 1 h at 800 °C (1472 °F) || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
SIGMA (N): solid, Morton et al. || quenched from 1500 °C (2732 °F), aged 5 h at 800 °C (1472 °F) || -248.1 °C (-414.7 °F) to 25 °C (77 °F)
return to listing
Nb4C3
D (N*): solid || cubic, Pm-3m || room temperature value
return to listing
Nb90Mo10H14.8 (New)
RHO : solid || -33 °C (-28 °F) to 70 °C (158 °F)
SIGMA : solid || -33 °C (-28 °F) to 70 °C (158 °F)
return to listing
NdAl2
TC (N): solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
NdCoO3
D (N*): solid || cubic || room temperature value
D (N*): solid || orthorhombic || room temperature value
return to listing
NdFe4Sb12
D (N*): solid || cubic || room temperature value
return to listing
NdPO4
D (N*): solid || hexagonal, P6_222 || room temperature value
D (N*): solid || monoclinic, P21/c || room temperature value
return to listing
NH4Br
E (N): solid || -36 °C (-33 °F) to 47 °C (116 °F)
G (N): solid || -36 °C (-33 °F) to 47 °C (116 °F)
v (N): solid || -36 °C (-33 °F) to 47 °C (116 °F)
K (N): solid || -36 °C (-33 °F) to 47 °C (116 °F)
return to listing
NH4ClO4
D (N*): solid || orthorhombic, Pnma || room temperature value
D (N*): solid || orthorhombic, Pna21 || room temperature value
return to listing
NH4HF2
D (N*): solid || orthorhombic, Pmna || room temperature value
return to listing
(NH4)2SO4
D (N*): solid || orthorhombic, Pna21 || room temperature value
D (N*): solid || orthorhombic, Pnma || room temperature value
return to listing
Ni - 20 Cu (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Ni - 30 Cu (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Ni - 40 Cu (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Ni - 0.5 Cu (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Ni - 3 Cu (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Ni - 10 Cu (wt %)
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
Ni - 8.5 Mo - 7 Ta - 6 Al (wt %) (New)
D (*): solid || room temperature value
CRS : 3% total strain, single crystal [001] orientation || tested at 1040 °C (1904 °F) || 2.5 h to 21 h
CRS : 3.5% total strain, single crystal [001] orientation || tested at 1040 °C (1904 °F) || 7 h to 33 h
CRS : 4% total strain, single crystal [001] orientation || tested at 1040 °C (1904 °F) || 10 h to 45 h
CRS : 5% total strain, single crystal [001] orientation || tested at 1040 °C (1904 °F) || 20 h to 70 h
IC : tested at 1040 °C (1904 °F), total strain, single crystal [001] orientation || 10 h || 0 to 0.39 mm/mm strain
IC : tested at 1040 °C (1904 °F), total strain, single crystal [001] orientation || 30 h || 0 to 0.61 mm/mm strain
IC : tested at 1040 °C (1904 °F), total strain, single crystal [001] orientation || 70 h || 0 to 0.18 mm/mm strain
IC : tested at 1040 °C (1904 °F), total strain, single crystal [001] orientation || 100 h || 0 to 0.146 mm/mm strain
CRR : single crystal [001] orientation || tested at 1040 °C (1904 °F) || 1.05 x 10-7/s to 3.3 x 10-7/s
return to listing
Ni - 1 Pd - 0.5 Fe (at %) (New)
RHO : solid || annealed || -243.1 °C (-405.7 °F) to 0 °C (32 °F)
SIGMA : solid || annealed || -243.1 °C (-405.7 °F) to 0 °C (32 °F)
return to listing
Ni - 1 Pd - 2 Fe (at %) (New)
RHO : solid || annealed || -243.1 °C (-405.7 °F) to 0 °C (32 °F)
SIGMA : solid || annealed || -243.1 °C (-405.7 °F) to 0 °C (32 °F)
return to listing
Ni - 1.7 Pd (wt %)
RHO (N): solid || annealed || -243.1 °C (-405.7 °F) to 0 °C (32 °F)
SIGMA (N): solid || annealed || -243.1 °C (-405.7 °F) to 0 °C (32 °F)
return to listing
NiB
D (N*): solid || orthorhombic, Cmcm || room temperature value
return to listing
Ni3B
D (N*): solid || orthorhombic, Pnma || room temperature value
return to listing
Nickel 200
E (R): solid || -273.1 °C (-459.7 °F) to 1050 °C (1922 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 500 °C (932 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 500 °C (932 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 500 °C (932 °F)
return to listing
Nickel
E (R): solid || -273.1 °C (-459.7 °F) to 1050 °C (1922 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 500 °C (932 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 500 °C (932 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 500 °C (932 °F)
SSCC (N): 0.0005/s || tested at 700 °C (1292 °F) || 0.18 to 0.8 mm/mm strain
SSCC (N): 0.001/s || tested at 700 °C (1292 °F) || 0.19 to 0.8 mm/mm strain
SSCC (N): 0.005/s || tested at 700 °C (1292 °F) || 0.5 to 0.8 mm/mm strain
SSCC (N): 0.01/s || tested at 700 °C (1292 °F) || 0.16 to 0.8 mm/mm strain
SSCC (N): 0.05/s || tested at 600 °C (1112 °F) || 0.24 to 0.8 mm/mm strain
SSCC (N): 0.05/s || tested at 650 °C (1202 °F) || 0.24 to 0.8 mm/mm strain
SSCC (N): 0.05/s || tested at 700 °C (1292 °F) || 0.24 to 0.8 mm/mm strain
SSCC (N): 0.05/s || tested at 750 °C (1382 °F) || 0.5 to 0.8 mm/mm strain
SSCC (N): 0.05/s || tested at 800 °C (1472 °F) || 0.5 to 0.8 mm/mm strain
SSCC (N): 0.05/s || tested at 850 °C (1562 °F) || 0.25 to 0.8 mm/mm strain
SSCC (N): 0.1/s || tested at 700 °C (1292 °F) || 0.19 to 0.8 mm/mm strain
return to listing
Ni0.595Nb0.405
RHO (N*): solid || amorphous || room temperature value
SIGMA (N*): solid || amorphous || room temperature value
S (N): solid || amorphous || -263.1 °C (-441.7 °F) to -5 °C (23 °F)
return to listing
Ni66Nb34 (New)
RHO (*): solid || amorphous || room temperature value
SIGMA (*): solid || amorphous || room temperature value
return to listing
Ni3S4
D (N*): solid || cubic, Fd-3m || room temperature value
return to listing
NiSe2
D (N*): solid || orthorhombic, Pnnm || room temperature value
return to listing
NiSi
D (N*): solid || cubic, P21-3 || room temperature value
D (N*): solid || orthorhombic, Pnma || room temperature value
D (N*): solid || orthorhombic, Pmmn || room temperature value
return to listing
NiTe
D (N*): solid || trigonal, R-3m || room temperature value
D (N*): solid || hexagonal, P63/mmc || room temperature value
return to listing
NiWO4
D (N*): solid || monoclinic, P2/c || room temperature value
return to listing
Ni37Zr63 (New)
RHO (*): solid || amorphous || room temperature value
SIGMA (*): solid || amorphous || room temperature value
return to listing
NpF3
D (N*): solid || hexagonal, P63/mmc || room temperature value
return to listing
PaBr4
D (N*): solid || monoclinic, P21/c || room temperature value
return to listing
PaCl5
D (N*): solid || monoclinic, C2/c || room temperature value
return to listing
Pb - 45 Bi - 20 Na (at %) (New)
TC : liquid || 350 °C (662 °F) to 800 °C (1472 °F)
return to listing
Pb - 70 Bi (at %) (New)
DLL : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
MTE : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
CTE : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
D : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
Vis : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
return to listing
Pb - 90 Bi (at %) (New)
DLL : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
MTE : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
CTE : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
D : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
Vis : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
return to listing
Pb - 20 Bi (at %) (New)
DLL : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
MTE : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
CTE : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
D : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
Vis : liquid || 350 °C (662 °F) to 1100 °C (2012 °F)
return to listing
PbB4O7
D (N*): solid || orthorhombic, Pmn21 || room temperature value
return to listing
Pb2SiO4
D (N*): solid || monoclinic || room temperature value
return to listing
PbSnF4
D (N*): solid || tetragonal, P4/nmm || room temperature value
return to listing
PbTe
E (R): solid || -273.1 °C (-459.7 °F) to 520 °C (968 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 520 °C (968 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 520 °C (968 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 520 °C (968 °F)
return to listing
Pd - 52 Fe (wt %) (New)
E : solid || no magnetic field || -186.1 °C (-303.1 °F) to 565 °C (1049 °F)
E : solid || 700 Oe magnetic field || -186.1 °C (-303.1 °F) to 565 °C (1049 °F)
return to listing
Pd - 44 Fe (wt %) (New)
E : solid || no magnetic field || -88 °C (-127 °F) to 540 °C (1004 °F)
E : solid || 700 Oe magnetic field || -88 °C (-127 °F) to 540 °C (1004 °F)
return to listing
Pd - 1 Ni - 5 Pt (at %) (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
Pd - 1 Ni - 0.1 Pt (at %) (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
Pd - 1 Ni - 0.5 Pt (at %) (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
Pd - 0.5 Ni (wt %) (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
Pd - 74 Pt (at %) (New)
D (*): solid || room temperature value
RHO : solid || annealed || -253.1 °C (-423.7 °F) to -183.1 °C (-297.7 °F)
SIGMA : solid || annealed || -253.1 °C (-423.7 °F) to -183.1 °C (-297.7 °F)
S : solid || -271.1 °C (-456.1 °F) to -163 °C (-262 °F)
return to listing
Pd - 93 Pt (at %) (New)
D (*): solid || room temperature value
RHO : solid || annealed || -253.1 °C (-423.7 °F) to -183.1 °C (-297.7 °F)
SIGMA : solid || annealed || -253.1 °C (-423.7 °F) to -183.1 °C (-297.7 °F)
S : solid || -271.1 °C (-456.1 °F) to -163 °C (-262 °F)
return to listing
Pd - 1 Pt (at %) (New)
D (*): solid || room temperature value
RHO : solid || annealed || -263.1 °C (-441.7 °F) to -183.1 °C (-297.7 °F)
SIGMA : solid || annealed || -263.1 °C (-441.7 °F) to -183.1 °C (-297.7 °F)
S : solid || -271.1 °C (-456.1 °F) to -183.1 °C (-297.7 °F)
return to listing
Pd - 8 Pt (at %) (New)
D (*): solid || room temperature value
RHO : solid || annealed || -263.1 °C (-441.7 °F) to -183.1 °C (-297.7 °F)
SIGMA : solid || annealed || -263.1 °C (-441.7 °F) to -183.1 °C (-297.7 °F)
S : solid || -271.1 °C (-456.1 °F) to -163 °C (-262 °F)
return to listing
Pd - 30 Pt (at %) (New)
D (*): solid || room temperature value
RHO : solid || annealed || -253.1 °C (-423.7 °F) to -183.1 °C (-297.7 °F)
SIGMA : solid || annealed || -253.1 °C (-423.7 °F) to -183.1 °C (-297.7 °F)
S : solid || -271.1 °C (-456.1 °F) to -183.1 °C (-297.7 °F)
return to listing
Pd - H (New)
DLL : solid || PdH0.72 || -243.1 °C (-405.7 °F) to 20 °C (68 °F)
DLL : solid || PdH0.82 || -243.1 °C (-405.7 °F) to 20 °C (68 °F)
DLL : solid || PdD0.7 || -243.1 °C (-405.7 °F) to 20 °C (68 °F)
MTE : solid || PdH0.72 || -243.1 °C (-405.7 °F) to 20 °C (68 °F)
MTE : solid || PdH0.82 || -243.1 °C (-405.7 °F) to 20 °C (68 °F)
MTE : solid || PdD0.7 || -243.1 °C (-405.7 °F) to 20 °C (68 °F)
CTE : solid || PdH0.72 || -243.1 °C (-405.7 °F) to 20 °C (68 °F)
CTE : solid || PdH0.82 || -243.1 °C (-405.7 °F) to 20 °C (68 °F)
CTE : solid || PdD0.7 || -243.1 °C (-405.7 °F) to 20 °C (68 °F)
return to listing
Pd80Si20 (New)
RHO : solid || at 100 kPa (14.5 psi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || at 3.5 GPa (508 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || at 4.2 GPa (609 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || at 5.3 GPa (769 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || at 7 GPa (1.02 Msi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO : solid || at 11.5 GPa (1.67 Msi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 100 kPa (14.5 psi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 3.5 GPa (508 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 4.2 GPa (609 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 5.3 GPa (769 ksi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 7 GPa (1.02 Msi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || at 11.5 GPa (1.67 Msi) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
PrAl2
TC (N): solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
PrCd (New)
RHO : solid || along the <110> axis || -269.1 °C (-452.5 °F) to -70 °C (-94 °F)
SIGMA : solid || along the <110> axis || -269.1 °C (-452.5 °F) to -70 °C (-94 °F)
S : solid || along the <110> axis || -269.1 °C (-452.5 °F) to -30 °C (-22 °F)
return to listing
Pr6O11
D (N*): solid || monoclinic || room temperature value
return to listing
PtS2
D (N*): solid || trigonal, P-3m1 || room temperature value
return to listing
PtSb2 (Te doped)
D (N*): solid || cubic || room temperature value
return to listing
R-409A (R-22/R-124/R-142b) (New)
D : liquid || -40 °C (-40 °F) to 71 °C (160 °F)
D : vapor || -40 °C (-40 °F) to 71 °C (160 °F)
TC : vapor || at 100 kPa (14.5 psi) || 33 °C (91 °F) to 152 °C (305 °F)
TC : vapor || at 250 kPa (36.3 psi) || 33 °C (91 °F) to 152 °C (305 °F)
TC : vapor || at 500 kPa (72.5 psi) || 33 °C (91 °F) to 152 °C (305 °F)
TC : vapor || at 750 kPa (109 psi) || 33 °C (91 °F) to 152 °C (305 °F)
TC : vapor || at 1 MPa (145 psi) || 33 °C (91 °F) to 152 °C (305 °F)
TC : vapor || at 1.33 MPa (193 psi) || 33 °C (91 °F) to 152 °C (305 °F)
TC : saturated vapor || 27 °C (80 °F) to 77 °C (170 °F)
SH : liquid || -40 °C (-40 °F) to 71 °C (160 °F)
SH : ideal gas || at 100 kPa (14.5 psi), atmospheric pressure || 20 °C (68 °F) to 100 °C (212 °F)
HC : liquid || -40 °C (-40 °F) to 71 °C (160 °F)
HC : ideal gas || at 100 kPa (14.5 psi), atmospheric pressure || 20 °C (68 °F) to 100 °C (212 °F)
VP : saturated liquid || -40 °C (-40 °F) to 71 °C (160 °F)
return to listing
R-404A (R-125/R-134a/R-143a) (New)
TC : liquid || at 2 MPa (290 psi) || 20 °C (68 °F) to 40 °C (104 °F)
TC : liquid || at 3 MPa (435 psi) || 20 °C (68 °F) to 60 °C (140 °F)
TC : liquid || at 4 MPa (580 psi) || 20 °C (68 °F) to 60 °C (140 °F)
TC : saturated liquid || at 4 MPa (580 psi) || 20 °C (68 °F) to 60 °C (140 °F)
TC : vapor || at 100 kPa (14.5 psi) || 40 °C (104 °F) to 155 °C (311 °F)
TC : vapor || at 750 kPa (109 psi) || 40 °C (104 °F) to 155 °C (311 °F)
TC : vapor || at 1.5 MPa (218 psi) || 60 °C (140 °F) to 155 °C (311 °F)
return to listing
R-507A (R-143a/R-125)
TC (N): liquid || at 1.6 MPa (232 psi) || 20 °C (68 °F) to 32 °C (89 °F)
TC (N): liquid || at 2.5 MPa (363 psi) || 20 °C (68 °F) to 52 °C (125 °F)
TC (N): liquid || at 3.5 MPa (508 psi) || 20 °C (68 °F) to 60 °C (140 °F)
TC (N): saturated liquid || at 3.5 MPa (508 psi) || 20 °C (68 °F) to 60 °C (140 °F)
TC (N): gas || at 100 kPa (14.5 psi) || 42 °C (107 °F) to 152 °C (305 °F)
TC (N): gas || at 500 kPa (72.5 psi) || 42 °C (107 °F) to 152 °C (305 °F)
TC (N): gas || at 1 MPa (145 psi) || 42 °C (107 °F) to 152 °C (305 °F)
TC (N): gas || at 1.25 MPa (181 psi) || 42 °C (107 °F) to 152 °C (305 °F)
TC (N): gas || at 1.5 MPa (218 psi) || 42 °C (107 °F) to 152 °C (305 °F)
TC (N): gas || at 1.75 MPa (254 psi) || 42 °C (107 °F) to 152 °C (305 °F)
return to listing
Rb - 25 Pb (at %) (New)
RHO : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
SIGMA : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
return to listing
Rb - 35 Pb (at %) (New)
RHO : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
SIGMA : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
return to listing
Rb - 45 Pb (at %) (New)
RHO : liquid || 603 °C (1117 °F) to 703 °C (1297 °F)
SIGMA : liquid || 603 °C (1117 °F) to 703 °C (1297 °F)
return to listing
Rb - 55 Pb (at %) (New)
RHO : liquid || 603 °C (1117 °F) to 703 °C (1297 °F)
SIGMA : liquid || 603 °C (1117 °F) to 703 °C (1297 °F)
return to listing
Rb - 65 Pb (at %) (New)
RHO : liquid || 603 °C (1117 °F) to 703 °C (1297 °F)
SIGMA : liquid || 603 °C (1117 °F) to 703 °C (1297 °F)
return to listing
Rb - 75 Pb (at %) (New)
RHO : liquid || 603 °C (1117 °F) to 703 °C (1297 °F)
SIGMA : liquid || 603 °C (1117 °F) to 703 °C (1297 °F)
return to listing
Rb - 85 Pb (at %) (New)
RHO : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
SIGMA : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
return to listing
Rb - 95 Pb (at %) (New)
RHO : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
SIGMA : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
return to listing
Rb - 10 Pb (at %) (New)
RHO : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
SIGMA : liquid || 500 °C (932 °F) to 600 °C (1112 °F)
return to listing
Rb3Bi
RHO (N): liquid || 500 °C (932 °F) to 700 °C (1292 °F)
SIGMA (N): liquid || 500 °C (932 °F) to 700 °C (1292 °F)
return to listing
Rb5Bi4 (New)
RHO : liquid || 450 °C (842 °F) to 650 °C (1202 °F)
SIGMA : liquid || 450 °C (842 °F) to 650 °C (1202 °F)
return to listing
Rh60B32Si8 (New)
D (*): solid || room temperature value
RHO : solid || amorphous || -196.1 °C (-321.1 °F) to 970 °C (1778 °F)
SIGMA : solid || amorphous || -196.1 °C (-321.1 °F) to 970 °C (1778 °F)
return to listing
Rh70B22Si8 (New)
D (*): solid || room temperature value
RHO : solid || amorphous || -188.1 °C (-306.7 °F) to 775 °C (1427 °F)
SIGMA : solid || amorphous || -188.1 °C (-306.7 °F) to 775 °C (1427 °F)
return to listing
RuGa3
D (N*): solid || tetragonal || room temperature value
return to listing
RuSe2
D (N*): solid || cubic, Pa-3 || room temperature value
return to listing
Samarium
RHO (N): solid || 0 °C (32 °F) to 935 °C (1715 °F)
RHO (N): liquid || 935 °C (1715 °F) to 1210 °C (2210 °F)
SIGMA (N): solid || 0 °C (32 °F) to 935 °C (1715 °F)
SIGMA (N): liquid || 935 °C (1715 °F) to 1210 °C (2210 °F)
return to listing
Sb2Pd
D (N*): solid || cubic, Pa-3 || room temperature value
return to listing
ScPd3 (New)
D (*): solid || room temperature value
SH : solid || -271.1 °C (-456.1 °F) to -259.1 °C (-434.5 °F)
HC : solid || -271.1 °C (-456.1 °F) to -259.1 °C (-434.5 °F)
return to listing
SIQUAL 8509
FSN (N): axial, 5 mm (0.197 inch), non-nitrided || tested at 20 °C (68 °F), R = -1, 0 mean stress, maximum stress || 150 cycles to 1 x 107 cycles
FSN (N): axial, 5 mm (0.197 inch), nitrided || tested at 20 °C (68 °F), R = -1, 0 mean stress, maximum stress || 130 cycles to 5 x 107 cycles
FSN (N): axial, 5 mm (0.197 inch), nitrided || tested at 20 °C (68 °F), -200 MPa (-29 ksi) mean stress, maximum stress || 3.8 x 104 cycles to 5 x 107 cycles
FSN (N): axial, 5 mm (0.197 inch), nitrided || tested at 20 °C (68 °F), 100 MPa (14.5 ksi) mean stress, maximum stress || 6 x 105 cycles to 5 x 107 cycles
FSN (N): axial, 5 mm (0.197 inch), nitrided || tested at 20 °C (68 °F), 200 MPa (29 ksi) mean stress, maximum stress || 7.7 x 105 cycles to 5 x 107 cycles
FSN (N): axial, 4 mm (0.157 inch), nitrided || tested at 20 °C (68 °F), R = -1, 0 mean stress, maximum stress || 135 cycles to 5 x 107 cycles
FSN (N): axial, 4 mm (0.157 inch), nitrided || tested at 20 °C (68 °F), -300 MPa (-43.5 ksi) mean stress, maximum stress || 1.4 x 106 cycles to 5 x 107 cycles
FSN (N): axial, 4 mm (0.157 inch), nitrided || tested at 20 °C (68 °F), -100 MPa (-14.5 ksi) mean stress, maximum stress || 6 x 105 cycles to 5 x 108 cycles
FSN (N): axial, 4 mm (0.157 inch), nitrided || tested at 20 °C (68 °F), 100 MPa (14.5 ksi) mean stress, maximum stress || 8 x 105 cycles to 5 x 107 cycles
FSN (N): axial, 3 mm (0.118 inch), nitrided || tested at 20 °C (68 °F), R = -1, 0 mean stress, maximum stress || 400 cycles to 5 x 107 cycles
FSN (N): axial, 3 mm (0.118 inch), nitrided || tested at 20 °C (68 °F), -275 MPa (-39.9 ksi) mean stress, maximum stress || 6 x 105 cycles to 5 x 108 cycles
return to listing
SmAl2 (New)
D (*): solid || room temperature value
TC : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
62 Sn - 38 Pb (wt %) (New)
Vis : liquid || 193 °C (379 °F) to 527 °C (980 °F)
return to listing
SnS2
D (N*): solid || trigonal, P-3m1 || room temperature value
D (N*): solid || hexagonal, P63mc || room temperature value
D (N*): solid || cubic, Fd-3m || room temperature value
return to listing
SrAl2O4
D (N*): solid || monoclinic || room temperature value
D (N*): solid || hexagonal || room temperature value
return to listing
SrCrSn(PO4)3
D (N): solid || 20 °C (68 °F) to 800 °C (1472 °F)
return to listing
Sr2IrO4
D (N*): solid || tetragonal || room temperature value
return to listing
SrSiO3
D (N*): solid || cubic || room temperature value
D (N*): solid || monoclinic || room temperature value
D (N*): solid || triclinic || room temperature value
return to listing
Sr2TaO3N
D (N): solid || 20 °C (68 °F) to 400 °C (752 °F)
return to listing
T6 (New)
D (*): solid || room temperature value
E : solid || 20 °C (68 °F) to 600 °C (1112 °F)
UTS : wrought material, rolling direction || 4-pt bending, triple tempered at 430 °C (806 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
UTS : wrought material, rolling direction || 4-pt bending, triple tempered at 460 °C (860 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
UTS : wrought material, rolling direction || 4-pt bending, triple tempered at 500 °C (932 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
UTS : wrought material, transverse direction || 4-pt bending, triple tempered at 430 °C (806 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
UTS : wrought material, transverse direction || 4-pt bending, triple tempered at 460 °C (860 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
UTS : wrought material, transverse direction || 4-pt bending, triple tempered at 500 °C (932 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
UTS : direct sintered material || 4-pt bending, triple tempered at 430 °C (806 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
UTS : direct sintered material || 4-pt bending, triple tempered at 460 °C (860 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
UTS : direct sintered material || 4-pt bending, triple tempered at 500 °C (932 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
YS : wrought material, rolling direction || 4-pt bending, triple tempered at 430 °C (806 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
YS : wrought material, rolling direction || 4-pt bending, triple tempered at 460 °C (860 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
YS : wrought material, rolling direction || 4-pt bending, triple tempered at 500 °C (932 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
YS : wrought material, transverse direction || 4-pt bending, triple tempered at 430 °C (806 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
YS : wrought material, transverse direction || 4-pt bending, triple tempered at 460 °C (860 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
YS : wrought material, transverse direction || 4-pt bending, triple tempered at 500 °C (932 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
YS : direct sintered material || 4-pt bending, triple tempered at 430 °C (806 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
YS : direct sintered material || 4-pt bending, triple tempered at 460 °C (860 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
YS : direct sintered material || 4-pt bending, triple tempered at 500 °C (932 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
%El : wrought material, rolling direction || 4-pt bending, triple tempered at 430 °C (806 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
%El : wrought material, rolling direction || 4-pt bending, triple tempered at 460 °C (860 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
%El : wrought material, rolling direction || 4-pt bending, triple tempered at 500 °C (932 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
%El : wrought material, transverse direction || 4-pt bending, triple tempered at 430 °C (806 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
%El : wrought material, transverse direction || 4-pt bending, triple tempered at 460 °C (860 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
%El : wrought material, transverse direction || 4-pt bending, triple tempered at 500 °C (932 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
%El : direct sintered material || 4-pt bending, triple tempered at 430 °C (806 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
%El : direct sintered material || 4-pt bending, triple tempered at 460 °C (860 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
%El : direct sintered material || 4-pt bending, triple tempered at 500 °C (932 °F) || 20 °C (68 °F) to 600 °C (1112 °F)
return to listing
Ta - 20 Nb (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Ta - 10 Nb (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Ta - 60 Nb (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Ta - 80 Nb (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Ta - 2.5 W (wt %)
K (N*): solid || room temperature value
return to listing
Ta - 10 W (wt %)
K (N*): solid || room temperature value
return to listing
Ta2N
D (N*): solid || trigonal, P-3m1 || room temperature value
return to listing
TbAl2 (New)
D (*): solid || room temperature value
TC : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
TbFeO3
D (N*): solid || orthorhombic || room temperature value
return to listing
Terbium
SH (R): solid || -63 °C (-82 °F) to 1357 °C (2474 °F)
HC (R): solid || -63 °C (-82 °F) to 1357 °C (2474 °F)
return to listing
ThN
D (N*): solid || cubic, Fm-3m || room temperature value
return to listing
Thorium
E (R): solid || -193.1 °C (-315.7 °F) to 500 °C (932 °F)
G (N): solid || -193.1 °C (-315.7 °F) to 67 °C (152 °F)
v (N): solid || -193.1 °C (-315.7 °F) to 67 °C (152 °F)
K (N): solid || -193.1 °C (-315.7 °F) to 67 °C (152 °F)
return to listing
ThS
D (N*): solid || cubic, Fm-3m || room temperature value
return to listing
Ti - 33 Al - 3 Mn (wt %) (New)
CRR : lamellar structure || tested at 700 °C (1292 °F) || 3 x 10-10/s to 1.6 x 10-8/s
CRR : lamellar structure || tested at 800 °C (1472 °F) || 5 x 10-9/s to 5 x 10-7/s
CRR : lamellar structure || tested at 900 °C (1652 °F) || 4.7 x 10-8/s to 5.3 x 10-7/s
CRR : duplex structure || tested at 700 °C (1292 °F) || 8 x 10-10/s to 4 x 10-8/s
CRR : duplex structure || tested at 800 °C (1472 °F) || 1.7 x 10-8/s to 5.5 x 10-7/s
CRR : duplex structure || tested at 900 °C (1652 °F) || 1.3 x 10-7/s to 2.1 x 10-6/s
return to listing
Ti - 48 Al - 2 W - 0.5 Si (at %) (ABB IMN-2) (New)
E : investment cast || 20 °C (68 °F) to 800 °C (1472 °F)
UTS : investment cast || nearly lamellar structure || 20 °C (68 °F) to 800 °C (1472 °F)
UTS : investment cast || duplex structure || 20 °C (68 °F) to 800 °C (1472 °F)
YS : investment cast || nearly lamellar structure || 20 °C (68 °F) to 800 °C (1472 °F)
YS : investment cast || duplex structure || 20 °C (68 °F) to 800 °C (1472 °F)
%El : investment cast || nearly lamellar structure || 20 °C (68 °F) to 800 °C (1472 °F)
%El : investment cast || duplex structure || 20 °C (68 °F) to 800 °C (1472 °F)
return to listing
Ti - 33.5 Al (wt %) (New)
CRR : lamellar structure || tested at 700 °C (1292 °F) || 1.3 x 10-11/s to 4 x 10-10/s
CRR : lamellar structure || tested at 800 °C (1472 °F) || 1.2 x 10-9/s to 1.5 x 10-7/s
CRR : lamellar structure || tested at 900 °C (1652 °F) || 2 x 10-8/s to 5 x 10-7/s
CRR : duplex structure || tested at 700 °C (1292 °F) || 1.3 x 10-10/s to 4 x 10-9/s
CRR : duplex structure || tested at 800 °C (1472 °F) || 3 x 10-9/s to 4 x 10-7/s
CRR : duplex structure || tested at 900 °C (1652 °F) || 1.05 x 10-7/s to 2 x 10-6/s
return to listing
Ti - 0.05 Pd (Grade 17)
E (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
NE (N): solid || stably oxidized || 122 °C (251 °F) to 823 °C (1513 °F)
return to listing
Ti - 0.15 Pd (Grade 7)
E (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
NE (N): solid || stably oxidized || 122 °C (251 °F) to 823 °C (1513 °F)
return to listing
Ti - 0.1 Ru (Grade 27)
E (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
NE (N): solid || stably oxidized || 122 °C (251 °F) to 823 °C (1513 °F)
return to listing
Ti - 40 V (wt %)
K (N*): solid || room temperature value
ST (N): liquid || 1610 °C (2930 °F) to 1927 °C (3500 °F)
return to listing
Ti - 26 V (wt %)
K (N*): solid || room temperature value
return to listing
Ti - 32 V (wt %)
K (N*): solid || room temperature value
return to listing
Ti Grade 1
E (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
NE (N): solid || stably oxidized || 122 °C (251 °F) to 823 °C (1513 °F)
return to listing
Ti Grade 3
E (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 800 °C (1472 °F)
NE (N): solid || stably oxidized || 122 °C (251 °F) to 823 °C (1513 °F)
return to listing
TiB
D (N*): solid || cubic, F-43m || room temperature value
D (N*): solid || orthorhombic, Pnma || room temperature value
return to listing
Ti50Be40Zr10 (New)
RHO : solid || amorphous || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || amorphous || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
TiI3
D (N*): solid || hexagonal, P63/mcm || room temperature value
D (N*): solid || orthorhombic, Pmmn || room temperature value
return to listing
Ti3O5
D (N*): solid || monoclinic || room temperature value
D (N*): solid || orthorhombic || room temperature value
return to listing
Ti3Sb (New)
D (*): solid || cubic A15 compound || room temperature value
RHO : solid || annealed || -265.1 °C (-445.3 °F) to 20 °C (68 °F)
SIGMA : solid || annealed || -265.1 °C (-445.3 °F) to 20 °C (68 °F)
return to listing
TlBiTe2
D (N*): solid || trigonal || room temperature value
return to listing
Tl3GeTe3
D (N*): solid || triclinic || room temperature value
return to listing
TlSbTe2
D (N*): solid || trigonal || room temperature value
return to listing
TmAl2 (New)
D (*): solid || room temperature value
TC : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
return to listing
TOPHET alloy A
UTS (N*): solid || room temperature value
YS (N*): solid || room temperature value
%El (N*): solid || room temperature value
return to listing
TOPHET alloy D
UTS (N*): solid || room temperature value
YS (N*): solid || room temperature value
%El (N*): solid || room temperature value
return to listing
UNS C64700
SSC (N): solution treated || tested at 20 °C (68 °F), 5.55 x 10-6/s || 0 to 0.2 mm/mm strain
SSC (N): solution treated, aged at 450 °C (842 °F) || tested at 20 °C (68 °F), aged 2 h, 5.55 x 10-6/s || 0 to 0.155 mm/mm strain
SSC (N): solution treated, aged at 450 °C (842 °F) || tested at 20 °C (68 °F), aged 25 h, 5.55 x 10-6/s || 0 to 0.1 mm/mm strain
SSC (N): solution treated, aged at 450 °C (842 °F) || tested at 20 °C (68 °F), aged 100 h, 5.55 x 10-6/s || 0 to 0.11 mm/mm strain
SSC (N): solution treated, aged at 450 °C (842 °F) || tested at 20 °C (68 °F), aged 800 h, 5.55 x 10-6/s || 0 to 0.135 mm/mm strain
UTS (N*): effect of aging time on room temperature value || aged 2 h || room temperature value
UTS (N*): effect of aging time on room temperature value || aged 25 h || room temperature value
UTS (N*): effect of aging time on room temperature value || aged 100 h || room temperature value
UTS (N*): effect of aging time on room temperature value || aged 800 h || room temperature value
YS (N*): effect of aging time on room temperature value || aged 2 h || room temperature value
YS (N*): effect of aging time on room temperature value || aged 25 h || room temperature value
YS (N*): effect of aging time on room temperature value || aged 100 h || room temperature value
YS (N*): effect of aging time on room temperature value || aged 800 h || room temperature value
FSN (N): solution treated || tested at 20 °C (68 °F), R = -1, axial, maximum stress || 1.2 x 105 cycles to 1 x 108 cycles
FSN (N): solution treated, aged at 450 °C (842 °F) || tested at 20 °C (68 °F), aged 2 h, R = -1, axial, maximum stress || 5 x 104 cycles to 1 x 109 cycles
FSN (N): solution treated, aged at 450 °C (842 °F) || tested at 20 °C (68 °F), aged 25 h, R = -1, axial, maximum stress || 1.01 x 105 cycles to 1 x 108 cycles
FSN (N): solution treated, aged at 450 °C (842 °F) || tested at 20 °C (68 °F), aged 800 h, R = -1, axial, maximum stress || 2.3 x 105 cycles to 1 x 108 cycles
FSN (N): solution treated, cold worked, aged 2 h at 450 °C (842 °F) || tested at 20 °C (68 °F), cold worked, aged 2 h, R = -1, axial, maximum stress || 1.8 x 105 cycles to 1 x 109 cycles
return to listing
UNS C71100
E (N): solid || 20 °C (68 °F) to 300 °C (572 °F)
return to listing
UNS C15760
E (N*): solid || room temperature value
G (N*): solid || room temperature value
v (N*): solid || room temperature value
K (N*): solid || room temperature value
return to listing
V - 5 Cr - 5 Ti (wt %)
E (R): annealed || -273.1 °C (-459.7 °F) to 1600 °C (2912 °F)
G (R): annealed || -273.1 °C (-459.7 °F) to 1600 °C (2912 °F)
v (R): annealed || -273.1 °C (-459.7 °F) to 1600 °C (2912 °F)
K (R): annealed || -273.1 °C (-459.7 °F) to 1600 °C (2912 °F)
return to listing
V - 15.1 Cr (wt %)
E (N*): solid || room temperature value
G (N*): solid || room temperature value
v (N*): solid || room temperature value
K (N*): solid || room temperature value
return to listing
V - 80 Cr (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
V - 40 Cr (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
V - 48 Ti (wt %)
K (N*): solid || room temperature value
return to listing
V - 9.4 Ti (wt %)
K (N*): solid || room temperature value
ST (N): liquid || 1677 °C (3050 °F) to 1927 °C (3500 °F)
return to listing
V - 14 Ti (wt %)
K (N*): solid || room temperature value
ST (N): liquid || 1690 °C (3074 °F) to 2027 °C (3680 °F)
return to listing
V - 24 Ti (wt %)
K (N*): solid || room temperature value
return to listing
V - 36 Ti (wt %)
K (N*): solid || room temperature value
return to listing
V - 40 Ti (wt %) (New)
D (*): solid || room temperature value
E (*): solid || room temperature value
G (*): solid || room temperature value
v (*): solid || room temperature value
K (*): solid || room temperature value
return to listing
Vanadium
E (R): annealed || -273.1 °C (-459.7 °F) to 1600 °C (2912 °F)
G (R): annealed || -273.1 °C (-459.7 °F) to 1600 °C (2912 °F)
v (R): annealed || -273.1 °C (-459.7 °F) to 1600 °C (2912 °F)
K (R): annealed || -273.1 °C (-459.7 °F) to 1600 °C (2912 °F)
CRR (N): 1.59 mm (0.0626 inch) sheet || tested at 600 °C (1112 °F) || 2.15 x 10-6/s to 1.34 x 10-4/s
CRR (N): 1.59 mm (0.0626 inch) sheet || tested at 700 °C (1292 °F) || 1.69 x 10-7/s to 1.63 x 10-4/s
CRR (N): 1.59 mm (0.0626 inch) sheet || tested at 900 °C (1652 °F) || 2 x 10-6/s to 1.4 x 10-4/s
CRR (N): 1.59 mm (0.0626 inch) sheet || tested at 1000 °C (1832 °F) || 1.85 x 10-7/s to 3.52 x 10-5/s
CRR (N): 1.59 mm (0.0626 inch) sheet || tested at 1260 °C (2300 °F) || 9.8 x 10-8/s to 1.1 x 10-4/s
return to listing
VB
D (N*): solid || orthorhombic, Cmcm || room temperature value
return to listing
V3B2
D (N*): solid || tetragonal, P4/mbm || room temperature value
return to listing
VOSO4
D (N*): solid || tetragonal, P4/n || room temperature value
return to listing
WSi2
RHO (N): deposited on <100> p-type Si || as-deposited || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO (N): deposited on <100> p-type Si || annealed at 550 °C (1022 °F) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO (N): deposited on <100> p-type Si || annealed at 800 °C (1472 °F) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO (N): deposited on <100> p-type Si || annealed at 1000 °C (1832 °F) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO (N): deposited on oxidized Si wafers || as-deposited || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
RHO (N): deposited on oxidized Si wafers || annealed at 550 °C (1022 °F) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA (N): deposited on <100> p-type Si || as-deposited || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA (N): deposited on <100> p-type Si || annealed at 550 °C (1022 °F) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA (N): deposited on <100> p-type Si || annealed at 800 °C (1472 °F) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA (N): deposited on <100> p-type Si || annealed at 1000 °C (1832 °F) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA (N): deposited on oxidized Si wafers || as-deposited || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA (N): deposited on oxidized Si wafers || annealed at 550 °C (1022 °F) || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
YAg (New)
RHO : solid || -253.1 °C (-423.7 °F) to 527 °C (980 °F)
SIGMA : solid || -253.1 °C (-423.7 °F) to 527 °C (980 °F)
return to listing
YCo2 (New)
D (*): solid || room temperature value
RHO : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
SIGMA : solid || -269.1 °C (-452.5 °F) to 20 °C (68 °F)
S : solid || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
return to listing
Y4Co3 (New)
RHO : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
SIGMA : solid || annealed || -269.1 °C (-452.5 °F) to 0 °C (32 °F)
S : solid || -269.1 °C (-452.5 °F) to 10 °C (50 °F)
return to listing
Y3RhSi3
D (N*): solid || monoclinic, C2/m || room temperature value
return to listing
Ytterbium
RHO (N): solid || 20 °C (68 °F) to 824 °C (1515 °F)
RHO (N): liquid || 824 °C (1515 °F) to 890 °C (1634 °F)
SIGMA (N): solid || 20 °C (68 °F) to 824 °C (1515 °F)
SIGMA (N): liquid || 824 °C (1515 °F) to 890 °C (1634 °F)
S (N): solid || 90 °C (194 °F) to 824 °C (1515 °F)
S (N): liquid || 824 °C (1515 °F) to 890 °C (1634 °F)
return to listing
Y10W2O21
D (N*): solid || orthorhombic, Pbcn || room temperature value
return to listing
YZn (New)
D (*): solid || room temperature value
SH : solid || -253.1 °C (-423.7 °F) to 25 °C (77 °F)
HC : solid || -253.1 °C (-423.7 °F) to 25 °C (77 °F)
return to listing
Zirconium
E (R): solid || -273.1 °C (-459.7 °F) to 1200 °C (2192 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 600 °C (1112 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 600 °C (1112 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 600 °C (1112 °F)
return to listing
57 Zn - 40 Al - 3 Cu (wt %) (New)
D (*): solid || room temperature value
UTS (*): as-cast || room temperature value
%El (*): as-cast || room temperature value
FSN : as-cast || tested at 20 °C (68 °F), R = -1, rotating beam, maximum stress || 3 x 104 cycles to 1 x 107 cycles
return to listing
59 Zn - 40 Al - 1 Cu (wt %) (New)
D (*): solid || room temperature value
UTS (*): as-cast || room temperature value
%El (*): as-cast || room temperature value
FSN : as-cast || tested at 20 °C (68 °F), R = -1, rotating beam, maximum stress || 1.4 x 104 cycles to 1 x 107 cycles
return to listing
43 Zn - 55 Al - 1.6 Si (wt %)
D (N*): solid || room temperature value
return to listing
78 Zn - 22 Al (wt %)
D (N*): solid || room temperature value
return to listing
80 Zn - 20 Al (wt %) (New)
D (*): solid || room temperature value
UTS (*): as-cast || room temperature value
%El (*): as-cast || room temperature value
FSN : as-cast || tested at 20 °C (68 °F), R = -1, rotating beam, maximum stress || 6 x 103 cycles to 1 x 107 cycles
return to listing
53 Zn - 47 Cu (wt %)
D (N*): solid || room temperature value
return to listing
62 Zn - 38 Cu (wt %)
D (N*): solid || room temperature value
return to listing
Zn - 43 Sb (at %) (New)
RHO : liquid || 570 °C (1058 °F) to 700 °C (1292 °F)
SIGMA : liquid || 570 °C (1058 °F) to 700 °C (1292 °F)
return to listing
Zn - 60 Sb (at %) (New)
RHO : liquid || 529 °C (984 °F) to 700 °C (1292 °F)
SIGMA : liquid || 529 °C (984 °F) to 700 °C (1292 °F)
S : liquid || 529 °C (984 °F) to 700 °C (1292 °F)
return to listing
Zn - 80 Sb (at %) (New)
RHO : liquid || 562 °C (1043 °F) to 700 °C (1292 °F)
SIGMA : liquid || 562 °C (1043 °F) to 700 °C (1292 °F)
S : liquid || 557 °C (1034 °F) to 700 °C (1292 °F)
return to listing
Zn - 10 Sb (at %) (New)
RHO : liquid || 504 °C (939 °F) to 700 °C (1292 °F)
SIGMA : liquid || 504 °C (939 °F) to 700 °C (1292 °F)
S : liquid || 512 °C (953 °F) to 700 °C (1292 °F)
return to listing
Zn - 30 Sb (at %) (New)
RHO : liquid || 534 °C (993 °F) to 700 °C (1292 °F)
SIGMA : liquid || 534 °C (993 °F) to 700 °C (1292 °F)
S : liquid || 547 °C (1016 °F) to 700 °C (1292 °F)
return to listing
ZnS
E (R): solid || -273.1 °C (-459.7 °F) to 1205 °C (2201 °F)
G (R): solid || -273.1 °C (-459.7 °F) to 27 °C (80 °F)
v (R): solid || -273.1 °C (-459.7 °F) to 27 °C (80 °F)
K (R): solid || -273.1 °C (-459.7 °F) to 27 °C (80 °F)
return to listing
Zn4Sb3 (Zn13Sb10) (Na & Mg doped)
RHO (N): liquid || 570 °C (1058 °F) to 700 °C (1292 °F)
SIGMA (N): liquid || 570 °C (1058 °F) to 700 °C (1292 °F)
return to listing
ZnWO4
D (N*): solid || monoclinic, P2/c || room temperature value
return to listing
Zr0.8Fe0.2 (New)
SH : solid || amorphous || -271.1 °C (-456.1 °F) to -253.1 °C (-423.7 °F)
HC : solid || amorphous || -271.1 °C (-456.1 °F) to -253.1 °C (-423.7 °F)
RHO : solid || amorphous || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
SIGMA : solid || amorphous || -269.1 °C (-452.5 °F) to 27 °C (80 °F)
return to listing
Zr64Ni36
RHO (N): solid || amorphous || 77 °C (170 °F) to 670 °C (1238 °F)
SIGMA (N): solid || amorphous || 77 °C (170 °F) to 670 °C (1238 °F)
S (N): solid || amorphous || -269.1 °C (-452.5 °F) to -35 °C (-31 °F)
return to listing
ZrV2 (New)
E : solid || -263.1 °C (-441.7 °F) to 20 °C (68 °F)
return to listing